316Ti Stainless Steel Coil
video

316Ti Stainless Steel Coil

316Ti and 329 Stainless Steel Coils are two of the most popular options when it comes to stainless steel coils. These coils are known for their durability, strength, and resistance to corrosion, making them ideal for a wide range of applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 316ti stainless steel coil in China. If you're going to wholesale high quality 316ti stainless steel coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

316Ti Stainless Steel Coil

Product Introduction

316Ti and 329 Stainless Steel Coils are two of the most popular options when it comes to stainless steel coils. These coils are known for their durability, strength, and resistance to corrosion, making them ideal for a wide range of applications.

 

chemical composition
C:≤0.08
Si≤1.00
Mn≤2.00
P≤0.035
S≤0.030
Ni 10.00~14.00
Cr 16.00~19.00
Mo 1.80~2.50
Ti≥0.2~0.70

5 207 700x500