STS316TI Stainless Steel Coils For Heat Exchanger , Inox 316Ti Stainless Steel Strip Coil
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of sts316ti stainless steel coils for heat exchanger , inox 316ti stainless steel strip coil in China. If you're going to wholesale high quality sts316ti stainless steel coils for heat exchanger , inox 316ti stainless steel strip coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
STS316TI Stainless Steel Coils For Heat Exchanger , Inox 316Ti Stainless Steel Strip Coil
Description
| Thickness: | 0.5-3.0mm | Width: | 1000-2000mm |
|---|---|---|---|
| Surface: | 2B BA | Type: | Cold Rolled |
| High Light: |
stainless steel coil stock,cold rolled stainless steel coil |
||
STS316TI Stainless Steel Coils For Heat Exchanger , Inox 316Ti Stainless Steel Strip Coil
STS316TI Coil For Heat Exchanger Manufacturer Inox 316Ti Stainless Steel Strip
Stainless Steel Grade 316Ti Cold Rolled Stainless Steel Strip Coil
1. Product Description
Under the years of experience in learning and designing, Bohome grows up gradually and have cooperated with sorts of world steel mill, including TISCO, POSCO, BAOSTEEL, ANGANG Steel, LISCO and etc. Meanwhile, we have a professional team for exporting and we will try our best to offer better customer service. We will fully able to meet high demand of global customers.
Besides, Bohome will also expand international partnerships and spread our concept, so that more people can enjoy and share excellent quality and reasonable price.
Main Grade:
201, 301, 304, 304L, 316, 316L, 316Ti,409L , 410, 420, 430, 436, 439, 904L,444
Application:
Petroleum, Chemical, Chemical fiber, Medical machinery, Smelting, Aerospace, Kitchenware, Ship-building, Environmental protection,
Heat exchangers, Pressure vessels, Condensers, Electricity, etc.
OEM Capability:
Under the strict control of quality,rading we introduce advanced equipment, and provide processing services, such as edge slitting, length cutting
and other further surface treatment. Product packing can be according to customer requirement.
Stainless steel grade 304 cold rolled stainless steel strip coil
2. Product Description:Stainless Steel Coil
The wrap is original package and 1 stainless steel coil stands in 1 container, and coil will be fixed with special stainless steel
wirerope, which can prevent coil from rolling during transport. Identification labels are tagged coils according to standard
specification or customer's instructions. Special packaging is available as per customer's requirement.
Stainless Steel Sheet
Packaging Details:
Stainless steel sheet will be wrapped with anti-rust paper and steel rings to prevent from damage.
Special packaging is available as customer's requirement.
Delivery Detail:
Shipped in 7 days after payment
Application:
1. Automotive:Automotive trim and molding/Difficult-to-form exhaust-system components, tubular manifolds, mufflers/Exhaust manifold and other
exhaust-system components, catalytic converter shells, clamps
2. Construction: Gutters and downspouts, roofing, siding
3. Kitchenware: Cooking utensils, dishwashers, ovens, range hoods, refrigerators, skewers
4. Chemical processing: Oil refinery equipment, oil burner and heater parts
5. Appliances: Hot water tanks, residential furnaces
6. Power generation: Heat Exchanger tubing;
7. Farming: Dry fertilizer spreaders/Farm animal pens
Facotory and their capacity of 300 series cold rolled coil:
| Main types of cold rolled stainless steel and origin | ||||
| Origin | Material Name | Surface | Thickness | Width |
| TISCO | 304/ 316/ 321/ 310/ 430/316Ti | 2B | 0.28-6.0 mm | 1000-2000 mm |
| BAOXIN | 304/ 316/ 321/ 310/ 430 | 2B | 0.25-3.0 mm | 1000-1219 mm |
| POSCO | 304/ 316/ 321/ 310/ 430 | 2B | 0.28-5.0 mm | 1000-1500 mm |
| JISCO | 304/ 316/ 321/ 310 | 2B | 0.30-3.0 mm | 1000-1500 mm |
| TSINGSHAN | 304/ 430 | 2B/ BA | 0.28-3.0 mm | 1000-1219 mm |
| 300 series stainless steel (mm) | ||||
| Original | Grade | Finish | Thickness | Width |
| TISCO | 304(L)/ 310/316(L)/321 | No.1/2B/BA/2D/Mirror/Etching | 0.28-16.0mm | 1000-2000mm |
| LISCO | 304(L)/316(L)/321 | No.1/2B/BA/2D/Mirror/Etching | 0.30-10.0mm | 800-1600mm |
| POSCO | 304(L)/ 310/316(L)/321 | No.1/2B/BA/2D/Mirror/Etching | 0.28-10.0mm | 1000-1550mm |
| JISCO | 304(L)/ 310/316(L)/321 | No.1/2B/BA/2D/Mirror/Etching | 0.30-10.0mm | 1000-1500mm |
Mechanical Data for 304/ 304L Stainless Steel Coil
| Stainless Steel Type | Minimum Tensile Strength (ksi) |
Minimum Yield Strength (0.2%, ksi) |
Hardness |
| 304 Stainless Steel | 75 | 30 | 88 |
| 304L Stainless Steel | 70 | 25 | 88 |
Chemistry and Mechanical Data For 300 Series Stainless Steel:
1.
| Chemical elements(%) | ||||||||||
| Grade | C | Si | Mn | P | S | Ni | Cr | Cu | N | Others |
| 304 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 8.0-11.0 | 18.00-20.00 | - | ≤0.10 | - |
| 310S | ≤0.08 | ≤1.50 | ≤2.00 | ≤0.045 | ≤0.030 | 19.00-22.00 | 24.00-26.00 | - | - | - |
| 316L | ≤0.030 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 10.00-14.00 | 16.00-18.00 | - | ≤0.10 | - |
| 321 | ≤0.08 | ≤1.00 | ≤2.00 | ≤0.045 | ≤0.030 | 9.00-12.00 | 17.00-19.00 | - | - | Ti 5C-0.70 |
2.
| Mechanical properties | |||||
| Grade | Yield Strength (Mpa) |
Tensile Strength (Mpa) |
Elongation (%) |
Rockers Hardness | Vickers Hardness |
| 304 | ≥205 | ≥520 | ≥40 | ≤90 | ≤200 |
| 310S | ≥205 | ≥520 | ≥40 | ≤90 | ≤200 |
| 316L | ≥175 | ≥480 | ≥40 | ≤90 | ≤200 |
| 321 | ≥205 | ≥520 | ≥40 | ≤90 | ≤200 |
The producing progress of stainless steel cold rolled:

| Item | Stainless steel all sheet(Hot rolled, cold rolled) |
| Standard | ASTM A240, GB/T3280-2007, JIS4304-2005, ASTM A167, EN10088-2-2005, etc., |
| Material | 310S, 310,316, 316L, 316Ti, 321, 321H, 347, 347H, 304, 304L |
| 201, 409, 409L, 410, 410S, 420, 430, 904L, Duplex, etc., | |
| Surface | 2B, 2D, BA, NO.1, NO.4,NO.8, 8K, mirror, checkered, embossed, hairline, sandblast, Brush, etching, etc., |
| Thickness | 0.03~10mm |
| Width | 1000mm,1219mm,1500mm,1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc., |
| Length | 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc., |
| Package | Standard export package, suit for all kinds of transportation, or as required. |
| Price term | Ex-Work, FOB, CNF, CFR, CIF, FCA, DDP, DDU, etc |
| Payment term | T/T, L/C |
| Price Term: | FOB/ CFR/ CIF |
| MOQ | 1 MT |
| Application | Stainless steel coil applies to construction field, ships building industry, petroleum, chemical industries, war and electricity industries, food processing and medical industry, boiler heat Exchanger, machinery and hardware fields, Stainless steel plate can be made according to the customers' requirements. |
3. Why Choose Us:
1. The company professional to supply stainless steel coil and plate.
2. We have slitting machine, cutting machine and polishing machine.
4. Business Details:
Shipping
1. Sea Freight:
Asia: 3-5 days
Americas: about 20 days
Middle East: about 20 days
2. Air Cargo (Size limited)
3. Land Transportation
4. Express (DHL, UPS...for samples )
Payment Methods
Stocks: T/T, L/C at sight
Futures: 30% T/T in advance, balance before shipment
FAQ
Q: Are you trading company or manufacturer ?
A: We are Manufacturing and processing enterprises.
Q: How long is your delivery time?
A: Generally, it is 3-10 days if the goods is in stock. If not, it may be 15-20 days. This is also based upon the quantity you need.
Q: Do you provide samples ? Is it free or extra?
A: Yes, we could offer the sample for free charge but do not pay the cost of freight.
Q: What are your payment terms?
A: Payment<=10000USD, 100% in advance.
Payment>=10000USD, 30% T/T in advance, balance before shipment.
Or 100% L/C


Hot Tags: sts316ti stainless steel coils for heat exchanger , inox 316ti stainless steel strip coil, China sts316ti stainless steel coils for heat exchanger , inox 316ti stainless steel strip coil suppliers, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils, 316L Stainless Steel Coil
You Might Also Like
Send Inquiry