Stainless Steel 410S (UNS S41008) Strip
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 410s (uns s41008) strip in China. If you're going to wholesale high quality stainless steel 410s (uns s41008) strip made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 410S (UNS S41008) Strip is a low carbon, non–hardening modification of Alloy 410 (UNS S41000) the general purpose 12% chromium martensitic stainless steel. The low carbon and a small alloy addition minimize austenite formation at high temperatures which restricts the alloys ability to harden. 410S remains soft and ductile even when rapidly cooled from above the critical temperature.

This non-hardening characteristic helps prevent cracking when the alloy is exposed to high temperatures or welded. Stainless Steel 410S is completely ferritic in the annealed condition. It exhibits adequate corrosion resistance similar to 410 and good oxidation resistance.
| Property | Specification |
|---|---|
| Material Type | 410S Stainless Steel |
| Thickness Range | 0.1 mm - 3.0 mm |
| Width Range | 5 mm - 600 mm |
| Hardness (HV) | ≤ 180 HV |
| Tensile Strength | ≥ 415 MPa |
| Yield Strength | ≥ 205 MPa |
| Elongation | ≥ 20% |
| Standard | ASTM A240, ASTM A666 |
| Surface Finish | 2B, 2D, BA, No.4, No.8 |
| Edge | Mill Edge, Slit Edge |
| Coil Weight | ≤ 5 tons |
| Application | Furnace tubes, heat exchangers, chemical equipment, etc. |

Steel Export and Supply Stainless steel 410S strips capabilities include:
Stainless steel 410S strips Annealed & Precision
Stainless steel 410S strips thickness-0.1mm to 6.00mm
Stainless steel 410S strips width-2.5mm to 1320mm (slit to close tolerances)
Steel provides Stainless steel 410S Cold rolled mill finish strips such as:
Stainless steel 410S strips 2D - cold rolled, heat treated, pickled.
Stainless steel 410S strips 2B - cold rolled, heat treated, pickled, skin passed on bright rolls.
Stainless steel 410S strips 2R(BA) - cold rolled, bright annealed
Stainless steel 410S strips HR - hot rolled, annealed
Hot Tags: stainless steel 410s (uns s41008) strip, China stainless steel 410s (uns s41008) strip suppliers, 316L Stainless Steel Coil, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils