Stainless Steel 410 Strip
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless steel 410 strip in China. If you're going to wholesale high quality stainless steel 410 strip made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Stainless Steel 410 Strip is the basic, general purpose martensitic stainless steel that is used for highly stressed parts and provides good corrosion resistance plus high strength and hardness. Stainless Steel 410 Strip contains a minimum of 11.5% chromium which is just sufficient enough to demonstrate corrosion resistance properties in mild atmospheres, steam, and many mild chemical environments.

It is a general purpose grade that is often supplied in the hardened but still machineable condition for applications where high strength and moderate heat and corrosion resistance are required. Stainless Steel 410 Strip displays maximum corrosion resistance when it's been hardened, tempered, and then polished.
STAINLESS STEEL 410 STRIP CHEMICAL PROPERTIES: -
| C | Mn | Si | P | S | Cr | Ni | |
|---|---|---|---|---|---|---|---|
| 410 | 0.15 max | 1.00 max | 1.00 max | 0.04 max | 0.03 max | min: 11.5 max: 13.5 |
0.50 max |
STAINLESS STEEL 410 STRIP MECHANICAL PROPERTIES:
| Grade | Tensile Strength ksi (MPa) min | Yield Strength 0.2% offset ksi (MPa) min | Elongation (% in 50mm) min | Hardness (Brinell) MAX | Hardness (Rockwell B) MAX |
|---|---|---|---|---|---|
| 410 | 65 (450) | 30 (205) | 20 | 217 | 96 |

STAINLESS STEEL 410 STRIP CORROSION RESISTANCE:
Good corrosion resistance to atmospheric corrosion, potable water, and to mildly corrosive environments
Its exposure to everyday activities (sports, food preparation) is generally satisfactory when proper cleaning is performed after exposure to use
Good corrosion resistance to low concentrations of mild organic and mineral acids
STAINLESS STEEL 410 STRIP WELDING CHARACTERISTICS:
Readily welded by all standard methods
To reduce the risk of cracking, it is suggested to pre-heat the work piece to 350 to 400°F (177 to 204°C)
Post weld annealing is recommended to retain maximum ductility
Hot Tags: stainless steel 410 strip, China stainless steel 410 strip suppliers, 316L Stainless Steel Coil, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils