Stainless 310 Steel Alloy Coil
video

Stainless 310 Steel Alloy Coil

Alloy 310 is not designed for service in wet corrosive environments. The high carbon content, which is present to enhance creep properties, has a detrimental effect on aqueous corrosion resistance. The alloy is prone to intergranular corrosion after long term exposure at high temperatures. However, due to its high chromium content (25%), Alloy 310 is more corrosion resistant than most heat resistant alloys.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of stainless 310 steel alloy coil in China. If you're going to wholesale high quality stainless 310 steel alloy coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

Alloy 310 is not designed for service in wet corrosive environments. The high carbon content, which is present to enhance creep properties, has a detrimental effect on aqueous corrosion resistance. The alloy is prone to intergranular corrosion after long term exposure at high temperatures. However, due to its high chromium content (25%), Alloy 310 is more corrosion resistant than most heat resistant alloys.

4 145

Property Value
Density 0.285 lbs/in³ (7.89 g/cm³)
Specific Heat 0.12 BTU/lb-°F (32 – 212°F), 502 J/kg-°K (0 – 100°C)
Modulus of Elasticity 28.5 x 10⁶ psi (196 GPa)
Thermal Conductivity 8.0 BTU/hr/ft²/ft/°F (10.8 W/m-°K)
Melting Range 2470 – 2555°F (1354 – 1402°C)
Electrical Resistivity 30.7 Microhm-in at 68°C, 78.0 Microhm-cm at 20°C

Fabrication Data

Alloy 310 can be easily welded and processed by standard shop fabrication practices.

Hot Forming

Heat uniformly at 1742 – 2192°F (950 – 1200°C). After hot forming a final anneal at 1832 – 2101°F (1000 – 1150°C) followed by rapid quenching is recommended.

Cold Forming

The alloy is quite ductile and forms in a manner very similar to 316. Cold forming of pieces with long-term exposure to high temperatures is not recommended since the alloy is subject to carbide precipitation and sigma phase precipitants.

Welding

Alloy 310 can be readily welded by most standard processes including TIG, PLASMA, MIG, SMAW, SAW and FCAW.