SS 420 Stainless Steel 2B Finish Coil
video

SS 420 Stainless Steel 2B Finish Coil

SS 420 2B finish coil is a martensitic chrome steel that gives smart corrosion resistance kind of like 410 and augmented strength and hardness. It is magnetic in each the toughened and hardened conditions. Maximum corrosion resistance is earned solely within the totally hardened condition.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of ss 420 stainless steel 2b finish coil in China. If you're going to wholesale high quality ss 420 stainless steel 2b finish coil made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

SS 420 2B finish coil is a martensitic chrome steel that gives smart corrosion resistance kind of like 410 and augmented strength and hardness. It is magnetic in each the toughened and hardened conditions. Maximum corrosion resistance is earned solely within the totally hardened condition.

4 176

Sure, here is a table outlining the specifications for SS 420 2B finish coil:

Specification Description
Grade SS 420
Thickness 0.3 mm - 6.0 mm
Width 1000 mm, 1219 mm, 1500 mm, Custom widths available
Length Coil
Edge Condition Mill Edge, Slit Edge
Surface Smooth, dull, reflective
Tensile Strength 620 MPa (min)
Yield Strength 345 MPa (min)
Standard ASTM A240/A240M
Application Cutlery, surgical instruments, valves, etc.