JIS SUS301 Stainless Steel Strip Coils CSP 1250mm Cold Rolled
video

JIS SUS301 Stainless Steel Strip Coils CSP 1250mm Cold Rolled

BA (Bright Annealed):Sometimes specified as “Bright Annealed Stainless Steel”, is a bright, cold-rolled, reflective finish retained by final annealing in a controlled atmosphere furnace. It is highly reflective and has the same appearance as a mirror. A final light rolling pass through polished rolls produces a smooth, reflective surface, excellent for decorative applications.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of jis sus301 stainless steel strip coils csp 1250mm cold rolled in China. If you're going to wholesale high quality jis sus301 stainless steel strip coils csp 1250mm cold rolled made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

JIS SUS301 Stainless Steel Strip Coils CSP 1250mm Cold Rolled

Description

Length: Customer's Request,in Coil Grade: 300 Series
Application: Construction,Kitchenware,Medical Instruments,Industry,Decoration Type: Cold Rolled Coil,Stainless Steel,Strip
Standard: ASTM,AISI,JIS,DIN,GB Width: 20mm-1250mm
Surface: BA,2B,2D Technique: Cold Rolled
Thickness: 0.15-3.0mm Edge: Mill Edge Slit Edge
Price Term: CIF CFR FOB EX-WORK Coil Weight: 1MT - 10MT
High Light:

Cold Rolled Stainless Steel Strip Coils

,

JIS SUS301 Stainless Steel Coils

,

1250mm Stainless Steel Coils

JIS G4313-2012 SUS301 CSP Temper 3/4H Vickers 370-430 Size: 0.6 x 158mm.x coil Stainless Steel Strip

301 Stainless Steel Strip Quick Details

Product Name 301 Stainless Steel Strip Supplier | 1.4310 Stainless Steel Strip
Grades 301/1.4310
Hardness 150HV-650HV
Thickness 0.03mm-3.0mm
Width Width:1.5mm-600mm
Edge Mill Edge, Slit Edge, Deburred Edge, Round Edge, V Type Edge
Quantity Tolerance ±10%
Paper Core Internal
Diameter
Ø 200mm,Ø300mm, Ø400mm, Ø500mm paper core, special internal diameter core and without paper core on
special request
Surface Finish NO.1, 2B, 2H(Rerolled Bright), BA, No.4, 8K (Mirror), HL (Hairline), Polishing Bright, etc
Applications Industrial springs
Conveyor belt
Connectors
Switch components
Aircraft components
Electric components
Precision stamping parts
Hardware
Packaging Wooden Pallet/Wooden Case
Payment Terms 30% TT deposit and 70% balance before shipment, 100% LC at sight
Delivery Time 7-10 working days
MOQ 5 Tons
Shipping Port Shanghai/Ningbo port
Sample The sample of 301 stainless steel strip is available
Remark 301 stainless steel strip can be customized

301 Stainless Steel Strip Features

Anti-corrosion

High Strength

Durable

Low Maintenance

Good Ductility

Excellent Surface Quality

Excellent for deep drawing with good ductility without intermediate annealing

301 Stainless Steel Strip Applications

Due to the high strength and excellent corrosion resistance, quality grade 301 stainless steel strip is widely used for following applications.

Industrial springs

Conveyor belt

Connectors

Switch components

Aircraft components

Electric components

Precision stamping parts

Hardware

301 Stainless Steel Strip Chemical Composition

The chemical components of grade 301 stainless steel strip is summarized in the following table:

Grade C Si Mn P S Cr Ni Mo
301 ≤0.15 ≤1.00 ≤2.00 ≤0.045 ≤0.030 16.00-18.00 6.00-8.00 –

301 Stainless Steel Mother Coil Mechanical Property

Below The Table Is For Your Reference:

Show 102550100 entries

Search:

Grade Standard Yield Strength
Rp0.2 (N/mm²)
Tensile Strength
Rm (N/mm²)
Elongation % Hardness
(HV)
Hardness
(HRB)
201 ASTM A240 ≥ 275 ≥ 520 ≥ 35 ≤ 260 ≤ 101
202 ASTM A240 ≥ 275 ≥ 520 ≥ 40 ≤ 218 ≤ 95
301 ASTM A240 ≥ 205 ≥ 520 ≥ 40 ≤ 200 ≤ 90
304 ASTM A240 ≥ 205 ≥ 515 ≥ 40 ≤ 210 ≤ 92
304L ASTM A240 ≥ 205 ≥ 520 ≥ 40 ≤ 200 ≤ 90
316L ASTM A240 ≥ 177 ≥ 480 ≥ 40 ≤ 200 ≤ 90
316Ti ASTM A240 ≥ 205 ≥ 520 ≥ 40 ≤ 200 ≤ 90
317L ASTM A240 ≥ 205 ≥ 515 ≥ 40 ≤ 218 ≤ 95
309S ASTM A240 ≥ 205 ≥ 515 ≥ 40 ≤ 218 ≤ 95
310S ASTM A240 ≥ 205 ≥ 520 ≥ 40 ≤ 200 ≤ 90

Showing 1 to 10 of 23 entries

 

301 Stainless Steel Strip Production Tolerance

 

Thickness(mm) Width<125mm 125mm≤Width<250mm 250mm≤Width<600mm
≥0.03-0.10 ±0.06T ±0.10T ±0.10T
≥0.10-0.15 ±0.01 ±0.015 ±0.020
≥0.15-0.20 ±0.015 ±0.020 ±0.025
≥0.20-0.25 ±0.015 ±0.020 ±0.025
≥0.25-0.30 ±0.018 ±0.025 ±0.030
≥0.30-0.40 ±0.020 ±0.025 ±0.030
≥0.40-0.50 ±0.025 ±0.030 ±0.040
≥0.50-0.60 ±0.030 ±0.030 ±0.040
≥0.60-0.80 ±0.030 ±0.040 ±0.040
≥0.80-1.00 ±0.030 ±0.040 ±0.050

 

301 Stainless Steel Strip Surface Finishes

Stainless steel strip is used in many industries. Many manufacturers are in fact, utilizing surface finishes for 301 stainless steel strip to achieve different results. If you are unfamiliar with surface finishes for 301 stainless steel strip, then this guide is for you.

BA (Bright Annealed):Sometimes specified as "Bright Annealed Stainless Steel", is a bright, cold-rolled, reflective finish retained by final annealing in a controlled atmosphere furnace. It is highly reflective and has the same appearance as a mirror. A final light rolling pass through polished rolls produces a smooth, reflective surface, excellent for decorative applications.

2B Finish:Cold rolled, heat treated, pickled, pinch passed. The most common cold rolled mill finish. Dull grey slightly reflective finish. Can be used in this condition or frequently is the starting point for some polished finishes.

2D Finish:A dull finish that is produced by cold rolling followed by annealing and descaling. Used in deep drawn objects which are often polished after fabrication.

Polishing Bright Finish:Mechanical Polishing: This process removes surface imperfections caused by grinding and other processing operations. In addition, it provides a moderate degree of luster to the surface which can be further enhanced by subsequent buffing operations using grease or oil emulsions with rouge or aluminum oxide compounds.

301 Stainless Steel Strip Edges Options

Many products managers and engineers have the trouble of 301 stainless steel strips edges.

In the actual operation process, due to the influence of steel strip hardness and unloading speed, it is difficult to effectively control the edge of the 301 foil strip.

However, after our technical personnel have studied for a long time, we have found a solution to this problem. The edge finishing of our 301 strips shall meet the requirements.

 

 

301 Stainless Steel Strip Hardness

301 stainless steel strip's hardness can be up to 600HV after precision production. Do you know the meaning of letter H in 301 stainless steel strip?

If you are the beginner of this area, you can benefit from this guide.

Let's keep reading:The Meaning Of Letter H In 301 Stainless Steel Strip.

The H and mechanical properties detailed information of grade 301 stainless steel strip is summarized in the following table:

Grade Status Hardness Yield Strength Tensile Strength Elogation
HV Mpa Mpa %

 

 

 

SUS301

ANN ≤218 ≥205 ≥520 ≥40
1/4H 250-310 ≥470 ≥780 ≥25
1/2H 310-370 ≥510 ≥930 ≥18
3/4H 370-430 ≥745 ≥1130 ≥5
FH 430-490 ≥1030 ≥1320 ≥4
EH 490-550 ≥1275 ≥1570 ≥3
SH ≥550 ≥1550 ≥1750 ≥1

What are The Advantages of Using 301 Stainless Steel Strips

The advantages of using 301 stainless steel strips are as follows:

1. High tensile strength, good toughness, stable quality, high and low temperature resistance, corrosion resistance

2. Different finishes such as bright annealing, matte annealing and black annealing are available

3. The surface is clean, smooth and beautiful

4. Good stretching performance to ensure the best processing performance of the product

JIS SUS301 Stainless Steel Strip Coils CSP 1250mm Cold Rolled 0JIS SUS301 Stainless Steel Strip Coils CSP 1250mm Cold Rolled 1

Hot Tags: jis sus301 stainless steel strip coils csp 1250mm cold rolled, China jis sus301 stainless steel strip coils csp 1250mm cold rolled suppliers, 2507 Stainless Steel Coil, 316L Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil

Send Inquiry

whatsapp

Phone

E-mail

Inquiry