For Pressure Vessel 0.1-8mm UNS S08904 904L Stainless Steel Coil Strip
video

For Pressure Vessel 0.1-8mm UNS S08904 904L Stainless Steel Coil Strip

Company Type: Agent Of TISCO Processing Technology: Cold Rolled Grade: 201 304 304L 316L 321 310S 317L 430 904L.etc Surface: 2B BA NO.4 Mirror 8K Standard: ASTM AISI GB DIN JIS EN Certificate: SGS/BV
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of for pressure vessel 0.1-8mm uns s08904 904l stainless steel coil strip in China. If you're going to wholesale high quality for pressure vessel 0.1-8mm uns s08904 904l stainless steel coil strip made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

For pressure vessel 0.1-8mm UNS S08904 904L Stainless Steel Coil Strip

Description

Company Type: Agent Of TISCO Processing Technology: Cold Rolled
Grade: 201 304 304L 316L 321 310S 317L 430 904L.etc Surface: 2B BA NO.4 Mirror 8K
Standard: ASTM AISI GB DIN JIS EN Certificate: SGS/BV
High Light:

stainless steel coil stock

,

304 stainless steel coil

For pressure vessel 0.6-10.0mm 904L stainless steel coils UNS S08904

Quick Detail

904L stainless steel coil

 

Name

904L stainless steel coil

Brand

AUTO KUMPO/TISCO BAOSTEEL


size

1219mm 1500mm or as required


surface

2B,No.1,BA, HL, 8K mirror, PVC coated

thickness

0.6mm-10.0mm

Certificate

SGS, BV


904L stainless steel coil,904L stainless steel sheet, 904L stainless steel plate
Coil weight: 5-27 ton
Coil type: Mill edge coil / slit edge coil

Description

used for pressure vessel 904L stainless steel coil, UNS S 08904 stainless steel coil

Details about our stainless steel sheet products:

1. 904L(S08904) stainless steel coil

2. Size: width: 1219mm 1500mm (slit edge)
1220-1265mm 1510-1575mm (mile edge)
thickness: 0.6-10.0mm (tolarance: 0%-5%)
3. Surface:original surface of our coil: 2B NO.1, we have a process factory, we can make the surface treatment like: BA HL mirror PVC coat.etc, we can also provide treatment like cutting , bending.etc

4. Mill of Origin: AUTO KUMPO TISCO BAOSTEEL.etc

5. Standard: GB JIS ASTM EN DIN AISI

6. packing: standard export seaworthy packing or as customer required.

Applications

Super austenitic stainless steel (904 l stainless steel plate) is a kind of low carbon high alloyed austenitic stainless steel, in dilute sulphuric acid have good corrosion resistance, specially designed for harsh environment corrosion conditions. Has high chromium content and plenty of nickel content, the addition of copper makes it have strong ability to resist acid, especially for chloride clearance corrosion and stress corrosion cracking are highly resistant, not easy appeared pitting spots and cracks, pitting resistance slightly better with other steel grade, good machinability and weldability, can be used for pressure vessels.

Specifications

used for pressure vessel 904L stainless steel coil, UNS S 08904 stainless steel coil

Size: 1219mm 1500mm or as required thickness: 0.6-10.0mm

Chemical Compostion of 904L

C

Si

Mn

P

S

Cr

Ni

Mo

Cu

<=0.03

<=1.00

<=2.00

<=0.035

<=0.03

18.00-20.00

23.00-25.00

3.0-4.0

4.0-5.0


National grade of 904L: China: 00Cr20Ni25Mo4.5Cu EN: 1.4539 ASTM N08904
Density(g/cm3) : 7.98

Our Capacity:

About us:strong technical force, complete product material specification

Specialize in :stainless steel pipe,stainless steel elbow,stainless steel pipe fitting

Main market:northern Europe, Western Europe, Mid East, Southeast Asia, South America

Management idea:do as good as our words, honesty, win-win, quality rooted, service supreme
For pressure vessel 0.1-8mm   UNS S08904 904L Stainless Steel Coil Strip 0For pressure vessel 0.1-8mm   UNS S08904 904L Stainless Steel Coil Strip 1For pressure vessel 0.1-8mm   UNS S08904 904L Stainless Steel Coil Strip 2
For pressure vessel 0.1-8mm   UNS S08904 904L Stainless Steel Coil Strip 3

Hot Tags: for pressure vessel 0.1-8mm uns s08904 904l stainless steel coil strip, China for pressure vessel 0.1-8mm uns s08904 904l stainless steel coil strip suppliers, 316L Stainless Steel Coil, 2507 Stainless Steel Coil, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil