Hot Rolling Steel Coils
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of hot rolling steel coils in China. If you're going to wholesale high quality hot rolling steel coils made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
advantage
(1) Hot rolling can significantly reduce energy consumption and cost. During hot rolling, the metal has high plasticity and low deformation resistance, which greatly reduces the energy consumption of metal deformation.
(2) Hot rolling can improve the processing performance of metals and alloys, that is, break the coarse grains in the casting state, significantly heal cracks, reduce or eliminate casting defects, transform the as-cast structure into a deformed structure, and improve the processing performance of the alloy.
(3) Hot rolling usually uses large ingots and large rolling reduction, which not only improves production efficiency, but also creates conditions for increasing the rolling speed and realizing the continuity and automation of the rolling process.
shortcoming
(1) After hot rolling, the non-metallic inclusions (mainly sulfides, oxides, and silicates) inside the steel are pressed into thin sheets, resulting in delamination (sandwiching). Delamination greatly deteriorates the tensile properties of the steel along the thickness direction and may cause interlaminar tearing as the weld shrinks. The local strain induced by weld shrinkage often reaches several times the yield point strain, which is much larger than the strain caused by load.
(2) Residual stress caused by uneven cooling. Residual stress is the internal self-balanced stress in the absence of external force. Hot-rolled steel sections of various sections have such residual stress. Generally, the larger the cross-section size of the section steel, the greater the residual stress. Although residual stress is self-balanced, it still has a certain impact on the performance of steel components under the action of external forces. For example, it may have adverse effects on deformation, stability, fatigue resistance, etc.
(3) Hot rolling cannot control the required mechanical properties of the product very accurately, and the structure and properties of hot-rolled products cannot be uniform. Its strength index is lower than cold work hardened products, but higher than fully annealed products, and its plasticity index is higher than cold work hardened products, but lower than fully annealed products.
(4) The thickness and size of hot-rolled products are difficult to control, and the control accuracy is relatively poor; the surface of hot-rolled products is rougher than that of cold-rolled products, and the Ra value is generally 0.5 to 1.5 μm. Therefore, hot rolled products are generally used as blanks for cold rolling processing.


FAQ
Q: Can you provide sample?
A: Yes, for regular sizes sample is free but buyer need to pay freight cost.
Q:How can I get a quotation from you?
A:You can leave us message, and we will reply every message in time. Or we may talk on line by trade manager. And you can also find our contact information on contact page.
Q: Do you accept the third party inspection?
A: Yes absolutely we accept.
Q:About product prices?
A:Prices vary from period to period due to cyclical changes in the price of raw materials.