Coated Galvanized Steel Coil PPGI
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of coated galvanized steel coil ppgi in China. If you're going to wholesale high quality coated galvanized steel coil ppgi made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Coated Galvanized Steel Coil PPGI
Product Description
coated galvanized steel coil ppgi
Specifications:
|
Raw material |
Pre-painted Steel Strips |
|
Thickness |
0.14-4.0mm |
|
Width |
600-1250mm |
|
Length |
max 4000mm, as your request |
|
Coil ID |
508/610mm |
|
Coil Weight |
4-12MT |
|
Surface Treatment |
Hot-dipped galvanized, alu-zinc,prepaninted |
| Logo | can be stamped as your request |
Packing:
Water proof paper covered with steel sheet on the top of product, bundled by steel strip with iron pallet
Applications:
Hot galvanized sheet and alloying galvanized sheet have excellent performance, possessing ideal com-prehensive properties of corrosion resistance,formation and coating. They are mainly used in building- roof,door,window,roller shutter door and suspended skeleton, autombiles- vehicle shell, chassis,door ,trunklid,oil tank, and ender,metallurgy-steel sash blank and color coated substrate, and electric equipments-refrigerator base and shell,freezer, and kitchen equipments.