2D Cold Rolled Steel Coil 1.4113 X6CrMo17-1 AISI 434 EN 10088-2 ISO 15156 With MTC 3.1
video

2D Cold Rolled Steel Coil 1.4113 X6CrMo17-1 AISI 434 EN 10088-2 ISO 15156 With MTC 3.1

ASTM 434 - EN 1.4113, similar to X6CrMoS17-1, is a stainless steel with excellent soft magnetic properties. Its high molybdenum and its low sulphur content provide a very good corrosion resistance in water, steam and other moderate aggressive media. It provides also a higher resistance against pitting corrosion. This Steel is mainly used in solenoid valves for pneumatic and hydraulic applications with higher requirements regarding corrosion resistance like in medical equipment.
Send Inquiry
Chat Now

As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.

Product Introduction

Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of 2d cold rolled steel coil 1.4113 x6crmo17-1 aisi 434 en 10088-2 iso 15156 with mtc 3.1 in China. If you're going to wholesale high quality 2d cold rolled steel coil 1.4113 x6crmo17-1 aisi 434 en 10088-2 iso 15156 with mtc 3.1 made in China, welcome to get free sample from our factory. Good service and reasonable price are available.

 

ASTM 434 - EN 1.4113, similar to X6CrMoS17-1, is a stainless steel with excellent soft magnetic properties. Its high molybdenum and its low sulphur content provide a very good corrosion resistance in water, steam and other moderate aggressive media. It provides also a higher resistance against pitting corrosion.

This Steel is mainly used in solenoid valves for pneumatic and hydraulic applications with higher requirements regarding corrosion resistance like in medical equipment.

product-750-750product-750-750product-750-750product-750-750

 

Stainless Steel Strip 1.4113, X6CrMo17-1 AISI 434 Cold Rolled Annealed EN 10088-2 ISO 15156 With MTC 3.1

 

Product name
Hot/Cold Rolled 0.1-2mm Thick 202 201 410 430 304 316 316L 436 431 434 436L 439 Mirror 2b Ba 8K No1 Surface Large Inventory of Stainless Steel Coil/Strip
Length As required
Steel grade 200 300 400 series
Thickness 0.5-100mm or as required
Standard ASTM A213,A312,ASTM A269,ASTM A778,ASTM A789,DIN 17456, DIN17457,DIN 17459,JIS G3459,JIS G3463,GOST9941,EN10216, BS3605,GB13296
Technique Hot Rolled , Cold Rolled , Extrusion
Surface Polishing
Thickness Tolerance ±0.01mm
Material 304,304L,309S,310S,316,316Ti,317,317L,321,347,347H,304N,316L, 316N,201,202
Application Widely used in petroleum,foodstuff,chemical industry,construction, electric power,nuclear,energy,machinery,biotechnology,paper making,shipbuilding,boiler fields.
Pipes also can be made according to the customer's required.
MOQ 1 ton , We can accept sample order.
Shipment Time Within 7-15 workdays after receiving deposit .
Export Packing Standard seaworthy export packing or according to the customers' request
Capacity 25000 Ton/Tons per Month

Essential details

 

ASTM 434 - EN 1.4113, similar to X6CrMoS17-1, is a stainless steel with excellent soft magnetic properties. Its high molybdenum and its low sulphur content provide a very good corrosion resistance in water, steam and other moderate aggressive media. It provides also a higher resistance against pitting corrosion.

This Steel is mainly used in solenoid valves for pneumatic and hydraulic applications with higher requirements regarding corrosion resistance like in medical equipment.

Application:

- Heat exchangers

- Acid and nitrogen oxide pipelines

- Acid storage tanks

- Acid transport tanks

- Dairy, fruit and vegetable and brewery industries

- Textile industry

- Household appliances

 

AISI 434 EN 1.4113 DIN X6CrMo17-1 Cold Rolled Stainless Steel Strip Coil

 

Ferritic stainless steel, AISI 434, UNS S43400, JIS SUS434, EN 1.4113, DIN X6CrMo17-1

 

Chemical composition ( weight % )

C Si Mn P S Cr Mo
0.08 max 1.00 1.00 0.040 0.030 16.00~18.00 0.9~1.40

 

Product forms

434 Stainless hot and cold-rolled steel coil, slit strip, cut sheets

2D Cold Rolled Steel Coil 1.4113 X6CrMo17-1 AISI 434 EN 10088-2  ISO 15156 With MTC 3.1 02D Cold Rolled Steel Coil 1.4113 X6CrMo17-1 AISI 434 EN 10088-2  ISO 15156 With MTC 3.1 12D Cold Rolled Steel Coil 1.4113 X6CrMo17-1 AISI 434 EN 10088-2  ISO 15156 With MTC 3.1 2

Tag:

cold rolled stainless steel coil,

 

stainless steel coil stock,

 

304 stainless steel coil

Hot Tags: 2d cold rolled steel coil 1.4113 x6crmo17-1 aisi 434 en 10088-2 iso 15156 with mtc 3.1, China 2d cold rolled steel coil 1.4113 x6crmo17-1 aisi 434 en 10088-2 iso 15156 with mtc 3.1 suppliers, 304 316 316l SS Cold Rolled Steel Coils, AISI430 Stainless Steel Foil, 2507 Stainless Steel Coil, 316L Stainless Steel Coil