Oriented Silicon Steel
As a leading supplier and manufacturer in China, GNEE Steel provides cost-effective nickel-based alloy products.
- Send E-mail: ss@gneesteel.com
Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of oriented silicon steel in China. If you're going to wholesale high quality oriented silicon steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Oriented silicon steel: It has strong directionality, the lowest iron loss value in the rolling direction, the highest magnetic permeability, and a higher magnetic induction value under a certain magnetization field. The silicon content of oriented silicon steel is about 3%. It also requires a low content of oxide inclusions in the steel and must contain certain inhibitors (MnS, A1N).
Non-oriented silicon steel: ferrosilicon alloy with very low carbon content. In the deformed and annealed steel sheet, its grains are distributed randomly. The silicon content of the alloy is 1.5% to 3.0%, or the sum of the silicon and aluminum content is 1.8% to 4.0%. The products are usually cold-rolled plates or strips, which are mainly used to manufacture motors and generators.
Cold Rolled Electrical Steel

| Thickness | GB/T2521-1996 | JIS C2553-86 | DIN 46400P.3 | AISI(1983) | GOST21427.1 | |||||
| mm | Designation | P1.7/50 | Designation | W1.7/50 | Designation | P1.7/50 | Designation | P1.7/50 | Designation | P1.7/50 |
| W/kg | W/kg | W/kg | W/kg | W/kg | ||||||
| 0.27 | ||||||||||
| 27Q140 | 1.4 | 27G140 | 1.4 | VM-89-27N | 1.4 | 3405-0.27 | 1.38 | |||
| 27Q130 | 1.3 | 27G130 | 1.3 | VM-130-278 | 1.3 | M4-0.27 | 1.27 | 3406-0.27 | 1.27 | |
| 27Q120 | 1.2 | 27G120 | 1.2 | M3-0.27 | 1.21 | 3407-0.27 | 1.2 | |||
| 27QG110 | 1.1 | 27P110 | 1.1 | M1H-0.27 | 1.09 | 3408-0.27 | 1.14 | |||
| 27QG100 | 1 | 27P100 | 1 | M0H-0.27 | 1.03 | 3409-0.27 | 1.08 | |||
| 0.3 | ||||||||||
| 30Q150 | 1.5 | 30G150 | 1.5 | 3404-0.30 | 1.5 | |||||
| 30Q140 | 1.4 | 30G140 | 1.4 | M5-0.3 | 1.39 | 3405-0.30 | 1.4 | |||
| 30Q130 | 1.3 | 30G130 | 1.3 | VM117-30P | 1.17 | M4-0.3 | 1.32 | 3406-0.30 | 1.33 | |
| 30QG130 | 1.3 | 30G120 | 1.2 | VM111-30P | 1.11 | M3-0.3 | 1.23 | 3407-0.30 | 1.25 | |
| 30QG120 | 1.2 | 30P110 | 1.1 | M2H-0.3 | 1.17 | 3408-0.30 | 1.2 | |||
| 30QG110 | 1.1 | M1H-0.3 | 1.11 | 3409-0.30 | 1.14 | |||||
| M0H-0.3 | 1.05 | |||||||||
Applications of Oriented Silicon Steel CRGO Coil:
1. Large power transformer
2. Medium & small power transformer
3. Distribution transformer
4. Reactor & magnetic amplifier
5. Audio transformer
6. Current & potential transformer
7. Ballast
8. Welding transformer
9. Magnetic switch core
Our GNEE Factory Packaging&Shipping

Hot Tags: oriented silicon steel, China oriented silicon steel suppliers, CRNGO Electrical Steel Coil