Gnee Super Alloy (Tianjin) Co., Ltd. is one of the most professional manufacturers and suppliers of cold rolled grain oriented silicon steel in China. If you're going to wholesale high quality cold rolled grain oriented silicon steel made in China, welcome to get free sample from our factory. Good service and reasonable price are available.
Silicon steel usually contains 2-4% silicon and is mainly divided into two types: oriented silicon steel and non-oriented silicon steel. Promisteel mainly provides oriented silicon steel, which can also be called oriented electrical steel, mainly used in producing large and small transformers. At the same time, we can also provide iron cores, if customers need to customize.
Cold-rolled grain-oriented silicon steel, also known as cold-rolled transformer steel, is an important ferrosilicon alloy used in the transformer (iron core) manufacturing industry. Its production process is complicated and its manufacturing technology is strict. It is mainly divided into common grain-oriented silicon steel (CGO) and high magnetic induction grain-oriented silicon steel (HiB).
| Product | Oriented silicon steel |
| Specification | Section shape: coil,strip,plate,sheet |
| Thickness: 2.0-6.0mm;customizable | |
| Width: 1219-2500mm;customizable | |
| Standard | ISO/ RoHS/ IBR/ AISI/ ASTM /GB/ EN / DIN /JIS |
| Material | 30Q130,B23P090,B30G120,B30G130,B35A300,35AW300,B50A250,B50A310 |
| Weight | 3-8 Tons |
| Package | ID:508-610mm |
| OD:Max 2000mm | |
| Min order | 5 tons, more quantity price will be lower |
| Payment terms | T/T, L/C |
| Deliver time | Within 7-30 days after deposit,base on quantity. |
| Others | We can do special orders as customer's requests. |
| We also can provide all kinds of steels coils. | |
| All the production process are made under the ISO9001:2008 strictly |
Cold rolled grain oriented electrical steel

Our Cold Rolled Grain Oriented Steel Advantages
There are two types of cold-rolled silicon steels strips: non-grain orientation and grain orientation. Usually, grain non-oriented cold-rolled strips are used as iron cores for motors or welding transformers; grain-oriented cold-rolled strips are used as iron cores for power transformers, pulse transformers, and magnetic amplifiers.
If the cold-rolled oriented strip is used, the performance is better. Using it instead of the hot-rolled strip or low-grade cold-rolled strip can reduce the power consumption of the transformer by 45%-50%, and the transformer's working performance is more reliable.
Cold rolled oriented silicon steel