2.4610 alloy plate is a low carbon nickel-molybdenum-chromium austenitic alloy, also known as Hastelloy C-4 alloy plate. Its chemical composition significantly reduces the carbon content and adjusts the proportion of silicon, iron and tungsten compared to earlier similar alloys.

The chemical composition of Hastelloy C4 hot rolled plate is as follows:
- Carbon (C): Maximum content 0.009%
- Silicon (Si): Maximum content 0.05%
- Manganese (Mn): Maximum content 1.0%
- Chromium (Cr): Content range 14.5% to 17.5%
- Nickel (Ni): Balance
- Molybdenum (Mo): Content range 14.0% to 17.0%
- Cobalt (Co): Maximum content 2.0%
- Titanium (Ti): Maximum content 0.7%
- Iron (Fe): Maximum content 3.0%
The physical properties of EN 2.4610 plate include:
Density: 8.64 g/cm³
Specific heat capacity: 427 J/kg·K
Thermal conductivity: 10~16.6 W/(m·K)
Modulus of elasticity: 205,000 MPa
Tensile strength: 690 MPa
Yield strength: 310 MPa
Elongation A5%: 40%
In addition, the alloy has a strong tendency to strain hardening. When the deformation rate reaches 15%, its hardening degree is about twice that of 18-8 stainless steel.
Application areas of Hastelloy C4
Chemical industry: used to treat highly corrosive media such as wet chlorine, oxidizing chlorides, chloride salts and various organic acids, halogen gases, etc.
Energy industry: used for wet phosphoric acid, HF acid production and flue gas desulfurization equipment, such as corrosion-resistant pipes, containers, towers, reactors, heat exchangers, etc.
Marine and land industries: used for subsea and deepwater offshore oil production systems, industrial air compressors, generators and nitrogen generators, etc.
EN 2.4610 plates show good cold and hot plasticity under appropriate manufacturing conditions, and show high stability at 650-1040℃, which improves the ability to resist intergranular corrosion.