Jun 04, 2025 Leave a message

What material is 4140, and what material does 4140 steel correspond to in China

What material is 4140, and what material does 4140 steel correspond to in China

 

I. What material is 4140

1. 4140 alloy structural steel, implementation standard: ASTM A29/A29M-04, is a medium hardenability steel, with good strength and good comprehensive mechanical properties after heat treatment, good processability and high yield rate. .4140 alloy structural steel is an alloy steel with a grade of 4140 and a carbon C of 33 to 48.

2. AISI 4140 steel is a low alloy steel containing chromium, molybdenum and manganese.

Due to its toughness, high fatigue strength, wear resistance and impact resistance, it is widely used in many industries and is an excellent material choice. Not many scores can match the versatility and practicality of 4140. 4140 chromium-molybdenum steel is provided in annealed or pre-hardened state.

info-500-500info-500-500

3. AISI4140 alloy structural steel is a common high-strength steel, corresponding to my country's GB standard steel number 42CrMo4. This steel has good mechanical properties and wear resistance, and has good gloss after grinding. This article will introduce the characteristics, chemical composition, mechanical properties and application examples of AISI4140 alloy structural steel.

4. What domestic materials does 4140 steel correspond to? Corresponding to the domestic 42CrMo grade steel, this material is a kind of alloy material with a carbon content of more than 33% and less than 48%, a hardness of up to 241HB, and very strong tensile strength.

5. C4140 is an important quenched and tempered structural steel that meets the American AISI standard.

Used to manufacture important structural workpieces, such as some military workpieces, large-size structural parts, etc. This steel has good processability, small processing deformation, good fatigue resistance, and is a medium-hardenability steel.

2. What materials does 4140 steel correspond to in China

1. What materials does 4140 steel correspond to in China? It corresponds to the domestic 42CrMo steel. This material is a kind of alloy material. Its carbon content is above 33% and below 48%. Its hardness is as high as 241HB. It also has very strong tensile strength.

2. AISI4140 steel plate is an alloy structural steel plate. AISI 414 steel is a low alloy steel containing chromium, molybdenum and manganese. American standard grade, it has a high carbon content, good balance of strength, toughness, wear resistance, impact resistance and heat treatment ability, but poor weldability. Corresponding to domestic 42CrMo.

3. In China, the corresponding steel to 4140 is 42CrMo steel. This steel has similar characteristics to 4140 and is also suitable for manufacturing molds, mechanical parts, automotive parts, etc. The two also have great similarities in chemical composition, mainly composed of carbon, silicon, manganese, sulfur, phosphorus, chromium and molybdenum.

4. Better answer: sae4140 is equivalent to domestic 42CrMo4 grade steel.

4140 alloy structural steel, implementation standard: ASTM A29/A29M-04, is a medium hardenability steel. After heat treatment, it has good strength and good comprehensive mechanical properties, good processability and high yield rate.

5. 4140 steel is equivalent to 40Cr steel in China. It is a heat-treated tool steel mainly composed of carbon, manganese, chromium, molybdenum and other elements. It has excellent mechanical properties, can withstand high temperatures, high strength, good toughness, and has impact resistance and corrosion resistance. It is an ideal material for the machinery manufacturing industry.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry