What is W. Nr 2.4856 material?
W.Nr. 2.4856 is the German material designation for Inconel alloy 625, which is widely used due to its high strength, excellent workability, and outstanding corrosion resistance. Its operating temperature range extends from cryogenic temperatures up to 980°C (1800°F). The strength of alloy 2.4856 is derived from the solid solution strengthening effect of molybdenum and niobium on the nickel-chromium matrix. Therefore, it does not require precipitation hardening treatment and can be processed into various practical product forms, including plates, coils, tubes, bars, and wires.
What material is 2.4856 equivalent to?
Material 2.4856, a German (Werkstoff) number, is equivalent to Alloy 625, also known by its UNS designation N06625, making it a high-strength, corrosion-resistant nickel-chromium-molybdenum alloy (NiCr22Mo9Nb) widely used in aerospace, marine, and chemical industries.
Is nickel alloy 2.4856 the same as Inconel 625?
Yes, nickel alloy 2.4856 and Inconel 625 are the same material; "2.4856" is its German material number (Werkstoff), while "Inconel 625" is the trade name for this specific nickel-chromium-molybdenum alloy, which has the Unified Numbering System (UNS) designation N06625.
alloy 2.4856 chemical composition
|
Grade |
C |
Mn |
Si |
P |
S |
Cu |
Fe |
Ni |
Cr |
|
Inconel 625 |
0.10 max |
0.50 max |
0.50 max |
– |
0.015 max |
– |
5.00 max |
58.00 min |
20.00 – 23.00 |
2.4856 Mechanical Properties
| Temper | Annealed (Grade1) | Solution-treated (Grade 2) | ||
|---|---|---|---|---|
| Tensile Rm | 120 | ksi (min) | 100 | ksi (min) |
| Tensile Rm | 827 | MPa (min) | 690 | MPa (min) |
| R.p. 0.2% Yield | 60 | ksi (min) | 40 | ksi (min) |
| R.p. 0.2% Yield | 414 | MPa (min) | 276 | MPa (min) |
| Elongation (2" or 4D gl) | 30 | % (min) | 30 | % (min) |
2.4856 Physical Properties (Room Temperature)
| Specific Heat (0-100°C) | 460 | J.kg-1.°K-1 |
| Thermal Conductivity | 14.8 | W.m -1.°K-1 |
| Thermal Expansion | 12.4 | μm/μm/°C |
| Modulus Elasticity | 207 | GPa |
| Electrical Resistivity | 10.3 | Ohm-cm |
| Density | 8.42 | g/cm3 |
Corrosion resistance:
Due to its high nickel, chromium, and molybdenum content, Inconel 625 exhibits excellent corrosion resistance, making it perform exceptionally well in harsh environments and resistant to pitting, crevice corrosion, and chloride stress corrosion cracking. Its corrosion resistance is far superior to traditional chromium-nickel-molybdenum stainless steels (1.4571; 1.4539; 1.4404, etc.), and it possesses extremely high resistance to intergranular corrosion, erosion, crevice corrosion, and stress corrosion cracking..

Welding: The Alloy 625 is easy to weld. The material 2.4831 is recommended as filler metal, taking into account the corresponding weld seam preparation for nickel alloys.
Forging: Before forging, the steel should be heated to a minimum of 950° C to 1150° C. This should be held for 60 minutes per 100 mm of decisive wall thickness. The forging process takes place at 1180° C to 950° C with subsequent rapid air or water cooling.
Are 2.4856 nickel-based alloys magnetic?
No, 2.4856 (Alloy 625) is generally non-magnetic, especially in its annealed (softened) state, due to its austenitic structure, making it suitable for applications requiring no magnetic interference, like in marine or chemical processing environments where strong corrosion resistance is also needed.
What is the difference between 2.4856 and 1.4404?
The difference between 2.4856 and 1.4404 lies in the fact that they are completely different materials: 1.4404 (AISI 316L) is a low-carbon stainless steel with good general corrosion resistance; while 2.4856 (Inconel 625) is a high-performance nickel alloy that offers superior strength and corrosion resistance in extreme high-temperature and corrosive environments (such as chemical processing). Therefore, 2.4856 has more specialized applications and is also more expensive.
At GNEE, we provide high-quality Inconel 625 in multiple forms, including sheets, plates, bars, rods, pipes, and tubes, meeting international standards such as ASTM, UNS, and ASME. Our products are certified with ISO, SGS, and BV, ensuring traceable quality.
We also offer services such as:
Cutting, bending, and shaping for custom components
Heat treatment to achieve desired hardness
Surface finishing for corrosion protection
Typical delivery lead time: 7–15 days, with secure packaging options including wooden crates, pallets, or bubble wrap.