What is the temperature rating for Inconel 600?

What is the temperature rating for Inconel 600?

 

 

Gnee Steel stocks Inconel Alloy 600 Nickel Alloy Plate in thicknesses from 3/16" (4.8mm) to 2" (50.8mm) for use in chemical and food processing equipment, paper mills, heat exchangers, and heat treating mufflers and retorts. Gnee Steel is a supplier of Inconel Nickel Alloy 600.

What is the temperature rating for Inconel 600?What is the temperature rating for Inconel 600?

Available Thicknesses of Inconel Alloy 600:
Inconel Alloy 600 (UNS N06600) is a nickel-chromium alloy designed for use in temperatures ranging from cryogenic to 2000°F (1093°C). Inconel Alloy 600 is non-magnetic and easily welded. The alloy is used in a variety of corrosion resistant applications. The high nickel content of Inconel Alloy 600 provides a degree of resistance to reducing environments, while the chromium content of the material provides resistance to less oxidizing environments. The high nickel content of the material provides excellent resistance to chloride stress corrosion cracking.

A versatile nickel-chromium-iron alloy with a unique combination of high temperature resistance up to 2000°F (1093°C) and excellent corrosion resistance.

Inconel Alloy 600 (UNS N06600) Specification Sheet Overview

W. Nr. 2.48161:

General Properties
Applications
Standards
Chemical Analysis
Physical Properties
Mechanical Properties
Corrosion Resistance
Heat Resistance
Manufacturing Data

Send Inquiry

whatsapp

Phone

E-mail

Inquiry