What is the temperature limit for Inconel 600?

What is the temperature limit for Inconel 600?

 

 

 

INCONEL Alloy 600

UNS Number N06600

Other common names: Alloy 600

W. NR 2.4816

ASTM B166, B167, B168

ASME SB166, SB167, SB 168

AMS 5540, 5665

600 alloy straight tubingIncoloy 600 pipe

Inconel 600 is a nickel-chromium alloy used for applications that require corrosion and high temperature resistance. This nickel alloy was designed for service temperatures from cryogenic to elevated temperatures in the range of 2000° F. It is non-magnetic, has excellent mechanical properties, and presents the desirable combination of high strength and good weldability under a wide range of temperatures. The high nickel content in Inconel 600 enables it to retain considerable resistance under reducing conditions, makes it resistant to corrosion by a number of organic and inorganic compounds, gives it excellent resistance to chloride-ion stress-corrosion cracking and also provides excellent resistance to alkaline solutions. Typical applications of this nickel alloy include the chemical, pulp and paper, aerospace, nuclear engineering and heat treating industries.

In what form is Inconel 600 Available at GNEE group?
Sheet
Plate
Bar
Pipe & Tube (welded & seamless)
Fittings
Elbows, tees, stub-ends, returns, caps, crosses, reducers, pipe nipples. etc.
Wire
What are the characteristics of Inconel 600?
Resistant to a wide range of corrosive media.
Virtually immune to chlorine ion stress corrosion cracking
Non-magnetic
Excellent mechanical properties
High strength and good weldability under a wide range of temperatures

Chemical Composition, %

Ni + Co Cr Fe C Mn S Si Cu

72.0 min

14.0-17.0

6.0-10.0

.15 max

1.00 max

.015 max

.50 max

.50 max

 

In what applications is Inconel 600 used?
Chemical industry
Aerospace
Heat treating industry
Pulp and paper industry
Food processing
Nuclear Engineering
Gas turbine components
Fabrication with Inconel 600
Alloy 600 can be both hot formed and cold formed using typical processes. Hot working should be performed between 1600° F and 2250° F avoiding any work between1200-1600° F because the ductility decreases in this temperature range. Welding Alloy 600 can be achieved via shielded metal-arc welding, TIG, and MIG.

ASTM Specifications

Pipe Smls Pipe Welded Tube Smls Tube Welded Sheet / Plate Bar Forging Fitting Wire

B167

B517

B163

B516

B168

B166

B564

B366

 

 

Mechanical Properties

Typical room temperature Tensile Properties of Annealed Material

Product Form Condition Tensile (ksi) .2% Yield (ksi) Elongation (%) Hardness (HRB)

Rod & Bar

Cold-Drawn

80-100

25-50

35-55

65-85

Rod & Bar

Hot-Finished

80-100

30-50

35-55

65-85

Tube & Pipe

Hot-Finished

75-100

30-50

35-55

–

Tube & Pipe

Hot-Finished

80-100

25-50

35-55

88 Max

Plate

Hot-Rolled

80-105

30-50

35-55

65-85

Sheet

Cold-Drawn

80-100

30-45

35-55

88 Max