What Is Nickel Alloy 201?
Nickel Alloy 201 is a wrought pure nickel grade with a carbon content of up to 0.02%, which is the key difference from Nickel 200. The low carbon level provides tough mechanical properties over a wide temperature range and keeps the material corrosion resistant in neutral to moderately reducing environments. Nickel 201 is ferromagnetic and offers high thermal and electrical conductivity compared with nickel-based alloys, stainless steels and low-alloy steels.
Why Low Carbon Matters
At temperatures above 600°F (316°C), the higher carbon content of Nickel 200 can cause graphitization, which weakens the material. Nickel Alloy 201, with carbon limited to 0.02%, avoids this problem and may therefore be considered for process service above 600°F where Nickel 200 is not recommended. This makes Alloy 201 the standard choice for caustic evaporators, synthetic fiber production and other elevated-temperature pure nickel applications.
Chemical Composition
Typical composition limits for Nickel Alloy 201 pipe are carbon 0.02% max, silicon 0.35% max, sulfur 0.01% max, manganese 0.35% max, iron 0.40% max, copper 0.25% max, with nickel 99.0% minimum. The balance is essentially pure nickel, which gives the alloy its characteristic resistance to caustic alkalis, chlorides and reducing media.
Mechanical and Physical Properties
In the annealed condition, Nickel 201 pipe typically shows a tensile strength of about 50 ksi, a 0.2% yield strength of about 12 ksi, and elongation of 35% in 2 inches. Density is 8.9 g/cm³ at room temperature, melting range is approximately 1435-1446°C, modulus of elasticity is about 207 kN/mm², electrical resistivity is 8.5 µΩ·cm at 20°C, coefficient of thermal expansion is 13.3 µm/m·°C from 20 to 100°C, and thermal conductivity is about 67.1 W/m·K at 20°C. These values place Alloy 201 among the most conductive and formable nickel materials available.
Pipe Specifications and Forms
Nickel Alloy 201 pipe is supplied as round tube from 4 mm to 200 mm outside diameter, square tube from 10x10 mm to 100x100 mm, and rectangular tube from 10x20 mm to 50x100 mm, with wall thickness from 0.6 mm to 6.0 mm and standard lengths of 1 to 6 meters, with custom lengths available. Common standards include ASTM, AISI, JIS, GB, DIN and EN, and surfaces can be black, bright polished, rough turned, matte, No.4 or BA. Production routes include hot rolled and cold rolled processing, with ISO, SGS or BV certification available on request.
FAQ
Q: What is the difference between Nickel 200 and Nickel 201 pipe?
A: The main difference is carbon content. Nickel 201 limits carbon to 0.02% max, which prevents graphitization in service above 600°F (316°C), where Nickel 200 is not recommended.
Q: Is Nickel 201 pipe magnetic?
A: Yes, Nickel 201 is ferromagnetic, unlike many austenitic nickel-based alloys.
Q: What environments does Nickel 201 resist?
A: It resists corrosion in neutral to moderately reducing media, including caustic alkalis, and is widely used in the production and handling of caustic soda.
Q: What sizes of Nickel 201 pipe are available?
A: Round tubes from 4 mm to 200 mm OD, square tubes from 10x10 mm to 100x100 mm and rectangular tubes from 10x20 mm to 50x100 mm, with wall thickness 0.6-6.0 mm and lengths of 1-6 meters or customized.
Q: What standards cover Nickel Alloy 201 pipe?
A: Pipe is commonly supplied to ASTM, AISI, JIS, GB, DIN and EN standards, with production by hot rolling or cold rolling.
Q: What are the typical mechanical properties of Nickel 201 pipe?
A: Annealed tensile strength is about 50 ksi, 0.2% yield strength about 12 ksi, and elongation 35% in 2 inches.