Feb 28, 2025 Leave a message

What is the difference between Monel and Inconel?

What is the difference between Monel and Inconel?

 

 

Inconel Vs Monel
Monel is a nickel copper alloy where the Inconel is a nickel chromium alloy. These materials have high corrosion resistance, high temperature resistance and are used in severe conditions. The different grades of monel and Inconel come with added elements such as aluminum which improve certain mechanical qualities to make them useful in unique applications.

Inconel Vs Monel Price
The nickel chromium composition is generally expensive than the nickel copper combination. However, depending on the amounts of nickel, chromium and copper in each different grade of the alloys, the prices can vary. In general, Inconel is more expensive than monel due to the high nickel chromium content.


Nickel Content In Inconel And Monel
Monel grades have up to 66% nickel and 31.5% copper in the composition. Inconel has 50% to 55% nickel in the composition. However, there are carbon, manganese, phosphorus, sulfur, silicon, molybdenum, columbium, titanium, aluminum, cobalt, boron, copper, tantalum, iron and 17-21% chromium additions to Inconel. Monel also has iron, manganese, carbon and silicon added to the composition.

Difference Between Inconel And Monel Corrosion Resistance
Inconel has higher oxidation resistance than monel where the Monel grades have resistance against sea water and reducing media such as hydrofluoric acid, sulfuric acid and alkalis. The corrosion resistance of Inconel under high temperatures makes it possible to be used in elevated temperature applications with the possibility of oxidation. The monel on the other hand can be used in sea water, marine, chemical and acid producing industries.


Inconel And Monel Alloy Melting Point
Both materials have similar melting points. The Inconel melting point ranes from 1290 degrees Celsius to 1350 degrees Celsius. Monel grades have melting points ranging from 1300 degrees Celsius to 1350 degrees Celsius. Although the melting points are similar the Monel alloys have higher toughness which make them useful for wear and tear resistant applications.


Inconel And Monel Density
Monel has higher densities than the Inconel due to the high nickel copper composition. Inconel has nickel but the chromium combination reduces the density a little bit lower than that of Monel. The monel grades have densities up to 8.8 grams per centimeter cube where the Inconel alloys have up to 8.2 grams per cubic centimeter. This makes the monel alloys a bit heavier than the Inconel variations.


Monel And Inconel Heat Treatment
The heat treatment of Inconel can be in the form of solution annealing which is to increase the temperature to higher levels and the allowing for rapid cooling. The cooling usually takes place underwater. Monel is heat treated by age hardening phase followed by a solution annealing similar to Inconel.


Difference Of Inconel And Monel Hardness
Inconel is harder than monel. The copper content in the monel material provides better ductility to the material. The Inconel is harder to machine, cutting and forming operations compared to the monel grades. The material composition of each specific grade can change the hardness of the material.


Inconel And Monel Temperature Range
Monel grades can perform from subzero temperatures to high temperatures as high as 480 degrees Celsius. The Inconel materials can perform from cryogenic temperatures all the way up to 982 degrees Celsius. The Inconel is more temperature resistant than monel.

What is the difference between Monel and InconelWhat is the difference between Monel and Inconel

Inconel And Monel Yield Strength
The Inconel materials have yield strengths ranging up to 460MPa and the tensile strengths ranging up to 760MPa. The monel grades have yield strengths up to 345MPa and tensile strengths up to 620MPa. The Inconel material is harder and stronger for making high strength accessories for high strength applications.

Equivalent Material Of Inconel

GradeUNS NoOld BritishEuronormGOSTJapanese JIS
BSEnNoAFNOR
Inconel 600 PipeN06600NA 13NiCr15Fe2.4816NC15FE11MМНЖМц 28-2,5-1,5NCF 600
Inconel 625N06625NA 21NiCr22Mo9Nb2.4856NC22DNB4MХН75МБТЮNCF 625
Inconel 601N06601NA 49NiCr23Fe2.4851NC23FeAXH60BTNCF 601
Incoloy 825N08825NA 16NiCr21Mo2.4858NFE30C20DUMЭП703

NCF 825

 

Mechanical Properties Of Inconel Grade

Tensile Strength (MPa) minYield Strength 0.2% Proof (MPa) minElongation (% in 50mm) minHardness
Rockwell B (HR B) maxBrinell (HB) max
Psi – 1,35,000 , MPa -930Psi – 75,000 , MPa – 51742.5––

 

Inconel Material Chemical Composition

InconelElement (% By Mass)
NiCrFeMoNbCoMnCuAlTiSiCSPB
60072.014.0–17.06.0–10.0   1.00.5  0.50.150.015  
61744.2–56.020.0–24.03.08.0–10.0 10.0–15.00.50.50.8–1.50.60.50.150.0150.0150.006
62558.020.0–23.05.08.0–10.03.15–4.151.00.5 0.40.40.50.10.0150.015 
69059.5309.2   0.350.010.02 0.350.0190.003  
71850.0–55.017.0–21.0Balance2.8–3.34.75–5.51.00.350.2–0.80.65–1.150.30.350.080.0150.0150.006
X-75070.014.0–17.05.0–9.0 0.7–1.21.01.00.50.4–1.02.25–2.75

 

Equivalent Material Of Monel

STANDARD

WERKSTOFF NR.

UNS

JIS

BS

GOST

AFNOR

EN

Monel 400

2.4360

N04400

NW 4400

NA 13

МНЖМц 28-2,5-1,5

NU-30M

NiCu30Fe

Monel K500

2.4375

N05500

–

–

–

–

–

 

Chemical Properties Of Monel

DesignationC%Co%Cr%Mo%Ni%V%W%Ai%Cu%Nb/Cb Ta%Ti%Fe%Sonstige Autres-Other %
Monel 4000.12---65.0---32.0--1.5Mn 1.0
Monel 4010.10---43.0---53.0--0.75Si 0.25; Mn 2.25
Monel 4040.15-  52.0-57.0--0.05rest/bal--0.50Mn 0.10; Si 0.10;S o.024
Monel 5020.10---63.0-17.0--2.5-3.5rest/bal-0.502.0Mn 1.5;Si 0.5; S 0.010
Monel K 5000.13---64.0--2.830.0-0.61.0Mn 0.8
Monel R 4050.15---66.0---31.0--

 

Monel Mechanical Properties

Tensile strength, Ultimate550 Mpa
Tensile strength, Yield240 Mpa
Elongation at Break48%

Send Inquiry

whatsapp

Phone

E-mail

Inquiry