UNS N07750 vs SS316: Composition, Properties and Selection

UNS N07750 and SS316 sit at opposite ends of the engineering alloy spectrum. One is an age hardenable nickel superalloy, the other a general-purpose austenitic stainless steel, so they differ sharply in strength, temperature capability and cost.

Composition Compared

UNS N07750 contains about 70 percent nickel, 14 to 17 percent chromium, 5 to 9 percent iron, 2.25 to 2.75 percent titanium, 0.4 to 1.0 percent aluminium and niobium. SS316 contains about 16 to 18 percent chromium, 10 to 14 percent nickel, 2 to 3 percent molybdenum and the balance iron.

The alloying level of X-750 is far higher, and its titanium and aluminium content allows precipitation hardening that stainless steel cannot use.

Strength and Hardening

SS316 is a solid-solution austenitic stainless steel that work hardens but cannot be strengthened by heat treatment. UNS N07750 is precipitation hardened by a controlled solution treatment and aging cycle, reaching much higher tensile and yield strength with good fatigue and relaxation resistance.

Where a component must carry high load, resist fatigue or act as a spring at temperature, X-750 is in a different performance class from 316.

High-Temperature Performance

SS316 retains useful strength to moderate temperatures and resists scaling, but its strength falls away quickly at high temperature. UNS N07750 keeps high strength to roughly 700 degrees C and resists oxidation and relaxation, which is why it is used in turbine and nuclear components.

For elevated temperature springs, bolts and clamps, X-750 is normally the material of choice.

Corrosion Resistance

SS316 offers good resistance to many atmospheric and moderate chemical environments and contains molybdenum for improved chloride pitting resistance. UNS N07750 offers good general corrosion resistance and oxidation resistance, but it is not intended as a substitute for high-molybdenum alloys in severe chloride or acid service.

Where the environment is dominated by aggressive chemicals, a dedicated corrosion alloy rather than either of these materials is usually required.

Cost and Selection

SS316 is inexpensive and widely available in every product form, making it the default choice where its strength and corrosion resistance are sufficient. UNS N07750 is far more costly and is specified only where high strength, fatigue resistance or high-temperature relaxation resistance is essential.

Consider X-750 for high-strength springs, fasteners and turbine or nuclear components, and SS316 for general structural, process and architectural duty.

Frequently Asked Questions

Q: Can SS316 be strengthened by heat treatment?
No. SS316 is austenitic and can only be strengthened by cold work, whereas UNS N07750 is precipitation hardened.

Q: Which material is stronger at high temperature?
UNS N07750, which retains high strength to roughly 700 degrees C, while SS316 loses strength much earlier.

Q: Why is X-750 used for springs?
Its age hardening gives high strength with good fatigue and relaxation resistance at temperature.

Q: Is SS316 cheaper than UNS N07750?
Yes, SS316 is far cheaper and more widely available because it contains much lower levels of nickel and no titanium or aluminium.

Q: Does either material suit severe chloride service?
Neither is intended for severe chloride pitting service, which normally requires a high-molybdenum corrosion alloy.