Jun 18, 2025 Leave a message

What is the difference between Inconel 718 and 750?

 
Inconel 718 VS 750 Alloy
 
Inconel 718 EFW Pipe
 

What is 718 in Inconel?

Inconel 718 is a niobium modified precipitation hardened nickel-iron alloy with a nominal composition of 50-55 wt% nickel, 17-21 wt% chromium, 4.8-5.5 wt% niobium, 2.8-3 wt% molybdenum, 0.65-1.15 wt% titanium, 1 wt% cobalt, and small amounts of aluminum (0.2-0.8 wt%) and iron (balance).

 

What is the difference between Inconel 718 and 750?

Compared to Inconel X-750, Inconel 718 has a higher chromium content. This makes Inconel 718 more resistant to oxidation than Inconel X-750. In addition, Inconel 718 alloy contains molybdenum, which is not found in X-750 alloy. The addition of molybdenum improves the resistance of Inconel 718 to reductive corrosion.

Inconel 718 welding
Inconel 718 seamless pipe
 

Is Inconel 718 stainless steel?

Inconel 718 is a precipitation-hardenable nickel-chromium alloy (not even in the same family as the iron-based stainless steels) that is approximately 50% nickel, 18% chromium, molybdenum, cobalt, and iron.

 

What is Inconel 718 alloy used for?

Inconel 718 alloy is commonly used in the aerospace industry. Engineers are constantly looking to improve the reliability and efficiency of engines, not to mention extend their service life. High-temperature alloys, especially 718 alloy, are widely selected for their balance between cost and performance.

Inconel 718

Inconel 718 and 750 Specifications

Chemical Composition: Inconel 718 vs Inconel X-750

Both alloys share a nickel-chromium base but differ in secondary elements that define their performance characteristics:

Element Inconel 718 Inconel X-750
Ni 50-55% 70% minimum
Cr 17-21% 14-17%
Fe Bal. 5-9%
Mo 2.8-3.3% –
Ti 0.65-1.15% 2.25-2.75%
Al 0.2-0.8% 0.4-1%
Nb 4.75-5.5% –
Co 1% max 1% max

Contact now

Mechanical Properties: Inconel 718 vs Inconel X-750

Property Inconel 718 Inconel X-750
Tensile Strength 1370 MPa 1100 MPa
Yield Strength 1030 MPa 780 MPa
Elongation 12-15% 15-20%
Hardness (Rockwell) B95-C36 B88-C32

Contact now

Performance in High-Temperature Environments

Inconel 718:
Inconel 718 is designed for medium to high temperature applications, but starts to lose mechanical properties above 700°C. Its good weldability makes it suitable for manufacturing processes that require high precision.

Inconel X-750:
Inconel X-750 can withstand temperatures up to 980°C and has excellent creep resistance. This makes it more suitable for manufacturing components such as turbine blades and nuclear reactor springs that need to be exposed to extreme temperatures for a long time.

Corrosion Resistance: Inconel 718 VS Inconel X-750

Both alloys exhibit excellent corrosion resistance:

Inconel 718 is more resistant to pitting, crevice corrosion, and stress corrosion cracking, especially in aqueous and sour environments. It is the preferred choice for offshore oil and gas applications.

Inconel X-750 has excellent oxidation resistance at high temperatures, but its resistance to chemical attack is inferior to Inconel 718.

Contact now

Inconel 718 vs Inconel X-750: Which is Better?

Criteria Inconel 718 Inconel X-750
Cost Higher cost More affordable
Machinability Easier to machine More challenging to machine
Weldability Excellent Less weldable
Corrosion Resistance Superior Moderate
Temperature Resistance Up to 700°C Up to 980°C
Applications High-strength, corrosive settings High-temperature environments

Choose Inconel 718:
If your application requires high strength, improved corrosion resistance, and moderate temperature performance, such as oil and gas or aerospace manufacturing.

Choose Inconel X-750:
If your application involves extremely high temperatures and long-term stresses, such as turbines, nuclear reactors, or high-temperature springs.

Contact now

In Conclusion:

Both Inconel 718 and Inconel X-750 are excellent materials, but their unique compositions and properties make them suitable for different applications. Inconel 718 excels in high-stress, corrosive environments, while Inconel X-750 is unmatched in high-temperature, creep-resistant conditions.

Gnee Steel has been focusing on the production and manufacturing of nickel alloys for more than a decade. We are the main supplier of corrosion-resistant alloys and other high-temperature alloy metals in China. With a professional technical team and after-sales service, we are able to provide high-quality Hastelloy, Incoloy, Inconel, Monel, duplex stainless steel and other alloy materials. These materials are supplied in wire, bar, plate, pipe, flange, forging and other forms to meet customer needs.

When choosing the right material for your project, consider the operating conditions, required mechanical properties and cost-effectiveness. If you are still unsure, contact Gnee Steel Group for expert advice to help you choose the alloy that best meets your needs.