Alloy 625 (UNS N06625) and Alloy C276 (UNS N10276) are both nickel-chromium-molybdenum materials, yet they are engineered for different jobs. One is a solid-solution strengthened grade that combines high as-annealed strength with excellent fatigue and welding behaviour; the other is a low-carbon, tungsten-bearing grade optimised for the most aggressive reducing chemical media. Comparing their chemistry first makes selection far easier than reading corrosion charts alone.
Chemistry and Phase Design
Alloy 625 is built on a nickel matrix of 58.0% minimum nickel, 20.0–23.0% chromium and 8.0–10.0% molybdenum, plus 3.15–4.15% niobium and tantalum. The niobium is the defining addition: it combines with molybdenum and distorts the atomic lattice, so the alloy reaches high strength in the annealed condition without any precipitation treatment. Alloy C276 keeps a comparable nickel base but shifts the balance towards molybdenum and tungsten: roughly 14.5–16.5% chromium, 15.0–17.0% molybdenum and 3.0–4.5% tungsten, with carbon held to 0.010% maximum and silicon to 0.08% maximum. Those tightly controlled carbon and silicon levels suppress grain-boundary carbide and intermetallic precipitation, which is why the alloy remains ductile after welding and in the heat-affected zone.
| Element, % | Alloy 625 / UNS N06625 | Alloy C276 / UNS N10276 |
|---|---|---|
| Nickel | 58.0 min | Balance |
| Chromium | 20.0–23.0 | 14.5–16.5 |
| Molybdenum | 8.0–10.0 | 15.0–17.0 |
| Tungsten | - | 3.0–4.5 |
| Niobium + Tantalum | 3.15–4.15 | - |
| Iron | 5.0 max | 4.0–7.0 |
| Carbon | 0.10 max | 0.010 max |
| Silicon | 0.50 max | 0.08 max |
Mechanical Properties and Strengthening Behaviour
Because Alloy 625 hardens by solid solution rather than by ageing, its properties are stable and reproducible even in heavy sections. Annealed bar to ASTM B446 is specified at 827 MPa minimum tensile strength, 414 MPa minimum yield strength and 30% minimum elongation, and the grade also retains useful toughness at cryogenic temperatures. Alloy C276 is not positioned as a structural high-strength grade: annealed bar to ASTM B574 carries a 690 MPa minimum tensile strength, 283 MPa minimum yield strength and 40% minimum elongation. The design intent is different – C276 trades some strength for maximum corrosion resistance and weldability in very aggressive chemistry. Both alloys work-harden rapidly, so forming operations need generous radii and inter-pass annealing, and both are austenitic, face-centred-cubic and non-magnetic in the annealed condition.
Corrosion Performance by Environment
In natural seawater and chloride-bearing process streams, both grades resist pitting and crevice attack, and both tolerate chloride stress corrosion cracking far better than 300-series stainless steels. The split appears in chemical service:
Reducing acids: C276 is the stronger choice for hydrochloric and sulfuric acid over wide concentration and temperature ranges, and for acetic and formic acid streams.
Oxidising and mixed media: Alloy 625 performs well in nitric acid and in mixed oxidising-reducing environments, and is widely used where chloride-induced localised attack must be avoided.
Chlorine and hypochlorite: C276 offers useful resistance to wet chlorine gas, chlorine dioxide and hypochlorite solutions, media that attack many nickel alloys.
Sour service: both grades are addressed in sour-service guidance such as NACE MR0175 / ISO 15156 for suitable product forms and conditions.
Physical Properties and Fabrication
| Property | Alloy 625 | Alloy C276 |
|---|---|---|
| Density, g/cm³ | 8.44 | 8.89 |
| Melting range, °C | 1290–1350 | 1323–1371 |
| Melting range, °F | 2350–2460 | 2415–2500 |
| Crystal structure | Austenitic, FCC | Austenitic, FCC |
| Magnetic response | Non-magnetic | Non-magnetic |
Both alloys are readily joined by gas tungsten arc and gas metal arc welding with matching nickel-base filler metals – ERNiCrMo-3 type filler for Alloy 625 and ERNiCrMo-4 type filler for Alloy C276. Clean surfaces, controlled heat input and inter-pass temperature limits matter more than for stainless steel, and C276 benefits from its very low carbon and silicon content when thick sections are welded without post-weld heat treatment. Machining is slow for both grades: high work-hardening rates call for rigid set-ups, sharp tooling and heavy, continuous cuts rather than light rubbing passes.
Standards, Product Forms and Availability
Alloy 625 is covered by ASTM B443 for sheet, plate and strip, ASTM B446 for bar and forgings, ASTM B444 for seamless tube and pipe, and ASTM B704 / B705 for welded tube and pipe, with fittings under ASTM B366 and aerospace coverage under AMS 5666 and AMS 5599. Its European designation is DIN 2.4856.
Alloy C276 is specified by ASTM B575 for plate, sheet and strip, ASTM B574 for bar, ASTM B622 for seamless pipe and tube, ASTM B619 for welded pipe, ASTM B626 for welded tube and ASTM B564 for forgings, with ASME SB equivalents widely referenced for pressure equipment, and DIN 2.4819 as the European designation.
Both grades are produced as seamless and welded tube and pipe, plate, sheet, strip, round, flat and hexagonal bar, wire and forgings, so one material family can cover a complete corrosive-service system.
FAQ
Q: Which alloy is stronger in the annealed condition?
Alloy 625, with a specified minimum yield strength of 414 MPa against 283 MPa for Alloy C276, because niobium and molybdenum distort its lattice and provide solid-solution strengthening.
Q: Can Alloy 625 replace Alloy C276 in hydrochloric acid service?
Only after testing. C276 carries much more molybdenum and adds tungsten, which is exactly what gives it the advantage in reducing acids such as hydrochloric and sulfuric acid.
Q: Why does Alloy C276 specify such a low carbon limit?
The 0.010% maximum carbon, paired with 0.08% maximum silicon, prevents grain-boundary carbide precipitation so welded joints and heat-affected zones keep their corrosion resistance and ductility.
Q: Are the two alloys interchangeable in seawater systems?
For many seawater components both work, but C276 is normally preferred where chlorides combine with reducing acids or chlorine, while Alloy 625 is often chosen where higher strength and fatigue resistance are also required.
Q: Which grade is easier to weld in thick sections?
C276, because its low carbon and silicon content reduce the risk of precipitation in the heat-affected zone and it usually needs no post-weld heat treatment.
Q: How do the two compare on cost?
Alloy C276 generally costs more, since it carries higher molybdenum and tungsten levels; Alloy 625 is the more economical route when its corrosion envelope suits the duty.