Jan 22, 2025 Leave a message

Datasheet-For-Inconel-601-1-6-(1)-(1).pdf

What is the cutting performance of Inconel 601?

The chemical composition of Inconel 601 contains high chromium and aluminum, which makes it have stronger oxidation resistance. This also makes the material harder during cutting, especially after heat treatment, the hardness will increase further.

Inconel 601
Therefore, it faces greater cutting force and higher cutting temperature during cutting, and the tool wears faster. It can be seen from the experimental data that under the condition of cutting speed of 100 m/min, the cutting force of Inconel601 is about 40% higher than that of traditional carbon steel.

Comparison of grinding performance of Inconel 690 and Inconel 601
Grinding is a processing method that cannot be ignored in metal cutting, especially in the processing of high hardness alloys. The difference in grinding performance between Inconel 690 and Inconel 601 is also obvious.

 

Grinding performance of Inconel 690
During grinding, Inconel 690 has a large grinding force due to its high hardness and toughness. Studies have shown that when using CBN (cubic boron nitride) grinding wheels, the grinding force of Inconel690 is relatively high, but the grinding temperature can still be effectively controlled, especially at low feed speeds. The surface roughness (Ra value) after grinding is usually between 0.3-0.5 μm, which meets the requirements of most applications.

Grinding performance of Inconel 601
Due to its high content of chromium and aluminum, the grinding performance of Inconel601 is usually difficult. During the grinding process, adhesion is prone to occur on the alloy surface, resulting in clogging of the grinding wheel. Therefore, it is particularly important to optimize the selection of grinding wheels and the use of cutting fluids. The use of diamond grinding wheels can effectively reduce the grinding temperature and maintain a longer grinding tool life. Experimental verification shows that when using appropriate coolant with high-speed grinding, the surface quality of Inconel601 is significantly improved, and the Ra value can be reduced to below 0.2 μm.

 

Cutting performance: Compared with Inconel601, Inconel690 requires lower cutting force and higher machining accuracy during cutting, but the tool life will be relatively short. Appropriately reducing the cutting speed and increasing the use of coolant are the keys to improving cutting efficiency.

Grinding performance: Both exhibit high grinding forces during grinding, but Inconel601 has greater tool loss during grinding due to its stronger heat resistance and oxidation resistance, and requires a more sophisticated grinding process and cooling system to ensure processing quality.

 

Send Inquiry

whatsapp

Phone

E-mail

Inquiry