Hastelloy C-276, also known as Alloy C-276, with the UNS designation N10276 and W. Nr. 2.4819, is a nickel-molybdenum-chromium alloy containing tungsten that is resistant to pitting, crevice corrosion and stress corrosion cracking and is suitable for use in harsh chemical processing environments.
Chemical composition of Hastelloy C276
Nickel: 58.0% - 63.0%
Chromium: 14.5% - 16.5%
Molybdenum: 15.0% - 17.0%
Rhenium: 0.1% - 0.2% (optional)
Iron: not more than 4.0%
Tungsten: not more than 3.5%
Physical and chemical properties of Hastelloy C276
| Density | Melting Point | Yield Strength (0.2%Offset) | Tensile Strength | Elongation |
|---|---|---|---|---|
| 8.89 g/cm3 | 1370 °C (2500 °F) | Psi – 52,000 , MPa – 355 | Psi – 1,15,000 , MPa – 790 | 40 % |
Delivery status of Hastelloy C276 steel pipe
Hot-rolled state: After high-temperature rolling, the inner and outer surfaces of the material maintain good smoothness.
Fine rolling state: Cold processing is performed to improve the dimensional accuracy and surface quality of the material.
Annealed state: After heat treatment, the material is more stable and the corrosion resistance is enhanced.
Pickling state: The surface iron oxide is removed by pickling to ensure the surface cleanness of the product.