Mar 20, 2025 Leave a message

What is the ASTM equivalent of Monel 400?

What is the ASTM equivalent of Monel 400?

 

 

Monel 400 Plate Specification

Specification ASTM B168 UNS N04400, ASME SB168
Sizes 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness 0.1mm to 100 mm Thk
Width 10-2500mm
Length 2m, 2.44m, 3m, or as required
ASTM ASTM B168
Finish Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.
Stock in form of Plate, Sheet, Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Clad Plate, Rolling Sheet, Flat Sheet, Rolling Plate, Flat Shim, Blank (Circle), hot rolled, cold rolled, annealed, soft annealed, descaled, sheared, tread plate, Checker Plate
Material JIS: N0, N2, N1, NW2200, NW2201, NW4400, NW5500, NW6002, etc
DIN:H-Ni99.96, H-Ni99.95, H-Ni99.92, H-Ni99.90, H-Ni99.5, H-Ni99, etc
ASTM Standard ASTM A162, GB/T2054, DIN177502002, ASTM B127,ASTM B435, ASTM B582, ASTM B575, ASTM B168, ASTM B443, ASTM B463, ASTM B626, ASTM B536, etc
Why choose Superior Steel Overseas

EN 10204/3.1B,

Raw Materials Certificate

100% Radiography Test Report

Third Party Inspection Report, etc

High special strength, high melt point

Excellent corrosive resistance,good thermal resistance

Customer support after-sales service

Huge Stock, Timely delivery

Strict Control from Raw Material to Finished Inconel 600 Plate

Free Quote, Inquiry answered within 24 hours

Inconel 600 profiling To provide a full profiling service we use numerous profiling methods including:

Laser Plate Cutting

Plasma Plate Cutting

Oxy-propane Flame Cutting

What is the ASTM equivalent of Monel 400What is the ASTM equivalent of Monel 400

ASTM B127 Plate Test Certificate
EN 10204/3.1B,
Raw Material Certificate
100% Radiographic Test Report
Third Party Inspection Report, etc.
ASTM B127 Plate Value Added Services
Mechanical Tests like Area Tensile
Hardness Test
Chemical Analysis - Spectroscopic Analysis
Positive Material Identification - PMI Test
Flattening Test
Micro and Macro Tests
Pitting Resistance Test
Expansion Test
Intergranular Corrosion (IGC) Test
ASTM B127 Plate Packaging Types
Bales (Hexagonal)
ASTM B152 Plate Packaging in Wooden Boxes
Crates (Steel/Wood)
Special crates for U-bends, separate for each radius
ASTM B152 Plate Packaging as per customer requirements

Chemical Composition Of Monel 400 Plates

Grade C Mn Si S Cu Fe Ni
Monel 400 0.30 max 2.00 max 0.50 max 0.024 max 28.00 – 34.00 2.50 max 63.00 min

Monel 400 Plates Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Monel 400 8.8 g/cm3 1350 °C (2460 °F) Psi – 80,000 , MPa – 550 Psi – 35,000 , MPa – 240 40 %

Monel 400 Plate Equivalent Grades

STANDARD WERKSTOFF NR. UNS
Monel 400 2.4360 N04400

Send Inquiry

whatsapp

Phone

E-mail

Inquiry