The Two Grades of Inconel 625
According to ASTM B446 it can be supplied in two different conditions:
Grade1
Inconel 625 Grade 1 is the product in Annealed condition. This is the most commonly stocked version, achieving a yield strength of 60ksi (414Mpa) for bars up to 4″ (101.6mm) diameter, and 50ksi (345MPa) for larger bars up to 10″ (254mm) diameter. The tensile strength minimum is 120ksi (827Mpa) and 110ksi (758Mpa) respectively.
Langley Alloys carries significant stock as solid bars between 5/8" (15.875mm) and 10" (254mm) diameter.
Our stock is also certified to API 6A CRA and NACE MR0175 / ISO 15156-3, and also AMS 5666.
Grade 2
Inconel 625 Grade 2 is supplied in the Solution Annealed condition. The main difference between Grade 2 and Grade 1 is the annealing temperature. In the case of Grade 1, the minimum annealing temperature is 1600F (871degC), whereas for Grade 2 it is now 2000F (1093degC). A further stabilisation anneal (1800F / 982degC) can be undertaken for the Grade 2 product to increase resistance to sensitisation from exposure at higher temperatures during operation, but is not essential.
By annealing at higher temperatures, the mechanical properties fall slightly compared with Grade 1. Instead of a yield strength of 60ksi/50ksi, it is now 40ksi for all sizes. Similarly, the minimum tensile strength is now 100ksi (690Mpa).
As the annealing temperature for Grade 2 is higher than that for Grade 1, it is possible to simply convert our existing Grade 1 stock to Grade 2 by arranging an additional heat treatment.
Inconel 625
Inconel 625 achieves fairly high strength through the addition of molybdenum and niobium to a nickel-chromium-based alloy, though not as high as Inconel 718. However, due to its high chromium and molybdenum content, it maintains good corrosion resistance even in the most corrosive environments.
Given its high nickel content (>58%), Inconel 625 is undoubtedly one of the more expensive alloys in our inventory. However, it maintains excellent performance at temperatures exceeding 800°C.
Besides specific applications at high temperatures, Inconel 625 is suitable for applications requiring extremely high corrosion resistance. Due to its very high molybdenum content (8-10%), Inconel 625 Grade 2 alloy has a pitting resistance equivalent (PREN) greater than 45.
This surpasses almost all alloy grades, and only a very few high-alloy grades can match it. It is virtually unaffected by corrosion in freshwater and exhibits good resistance to more corrosive oxidizing and non-oxidizing acids. For example, it is one of the few alloys suitable for handling or storing hydrochloric acid (a highly oxidizing environment).
Our factory
Our nickel-based alloy products originate from a modern precision manufacturing base. The factory is equipped with fully automated vacuum induction melting (VIM), electroslag remelting (ESR), and multi-directional forging hydraulic units, ensuring that every step from melting to forming meets aerospace-grade standards. Through a digital process control system, we achieve precise control over composition purity, grain size, and mechanical properties. Each batch of products is accompanied by traceable melting reports and third-party certifications (such as DNV-GL, ABS, aerospace standards, etc.), ensuring the authenticity and reliability of performance data.

Packaging and shipping
We adopt the highest industry standards for protective packaging: all rods/plates are treated with anti-rust protection and reinforced with waterproof film and wooden crates; precision components are packaged with custom foam dividers and vacuum sealing. Through our proprietary logistics coordination system, we promise that standard specification products will be prepared and shipped within 7-15 working days after order confirmation and technical details are finalized.