01.

What is Inconel 601 tubing? Learn more in this guide.

Inconel 601 tubing is a high-performance nickel-chromium-iron alloy designed for applications requiring excellent resistance to high-temperature oxidation and corrosion, as well as high mechanical strength. Its unique composition makes it a versatile material for use in harsh industrial environments.

02.

What is Inconel 601 used for?

In industrial furnaces, this alloy is used to manufacture radiant tubes, muffles, distillation retorts, flame shields, wire annealing tubes, woven wire conveyor belts, chain curtains, burner nozzles, and resistance heating elements.

info-800-400

Inconel 601 tubing is an alloy product composed of nickel, chromium, and iron. These products are suitable for general engineering applications, particularly those requiring heat and corrosion resistance. Inconel 601 tubing is also suitable for acidic aqueous environments.

The microstructure of Inconel 601 tubing conforms to ASTM B516 standards, making it a reliable solution. Due to its special structure, Inconel 601 tubing possesses high metallurgical stability. Furthermore, Inconel 601 contains nickel as the base alloy element, combined with chromium. All these elements give Inconel 601 excellent corrosion resistance and high-temperature performance.

 

info-665-296

Specification of Inconel 601 Pipe

Parameter Details
Standards ASTM B167, BS17 / ASME SB167, SB517
Dimensional ANSI/ASME B36.19M, ANSI/ASME B36.10M
Seamless Pipe Size 1/2″ NB – 16″ NB
Welded Pipe Size 1/2″ NB – 24″ NB
Outside Diameter 6.00 mm OD up to 914.4 mm OD, Sizes up to 24″ NB available Ex-stock, OD Size Steel Tubes available Ex-stock
Pipe Type Seamless / Welded / ERW / Fabricated / CDW / 100% X Ray Welded
Thickness Range SCH 5, SCH10, SCH 40, SCH 80, SCH 80S, SCH 160, SCH XXS, SCH XS
Pipes End Plain End, Beveled End, Treaded One End, TBE (Treaded Both Ends)
Value Added Services Cutting, Beveling, Polishing, Threading, Destructive, Non Destructive, Ultrasonic Testing

 

Equivalent Grades of Inconel 601 Pipe

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 601 2.4851 N06601 NCF 601 NA 49 XH60BT NC23FeA NiCr23Fe

 

Price List of Inconel Alloy 601 Pipe

Product Description Price in India (INR) Price in UK (GBP) Price in UAE (AED)
Inconel 601 Pipe 38 mm OD 5 mm Thk INR 7,034 76.18 GBP 363.28 AED
Inconel 601 Pipe (1-1/2" x Sch. 40s x 2,000 L) INR 31,984 346.41 GBP 1,651.87 AED
Inconel 601 Seamless Pipe (32.8" OD x 1.6" WT x 6.00 L) INR 35,613 385.72 GBP 1,839.29 AED
Inconel 601 Pipe (3/4" x Sch. 10s x 2,000 L) INR 12,632 136.82 GBP 652.40 AED

 

Schedule Chart of Inconel Alloy 601 Pipe

Nominal Pipe Size (IPS) Outer Diameter (O.D.) Available Schedules (SCH)
1/8" IPS .405" O.D. SCH 40, 80
1/4" IPS .540" O.D. SCH 10, 40, 80
3/8" IPS .675" O.D. SCH 10, 40, 80
1/2" IPS .840" O.D. SCH 5, 10, 40, 80, 160, XXH
3/4" IPS 1.050" O.D. SCH 10, 40, 80, 160, XXH
1" IPS 1.315" O.D. SCH 5, 10, 40, 80, 160, XXH
1-1/4" IPS 1.660" O.D. SCH 10, 40, 80, 160, XXH
1-1/2" IPS 1.900" O.D. SCH 10, 40, 80, 160, XXH
2" IPS 2.375" O.D. SCH 10, 40, 80, 160, XXH
2-1/2" IPS 2.875" O.D. SCH 10, 40, 80, 160, XXH
3" IPS 3.500" O.D. SCH 5, 10, 40, 80, 160, XXH
3-1/2" IPS 4.000" O.D. SCH 10, 40, 80, 160, XXH
4" IPS 4.500" O.D. SCH 10, 40, 80, 160, XXH
5" IPS 5.563" O.D. SCH 10, 40, 80, 160, XXH
6" IPS 6.625" O.D. SCH 5, 10, 40, 80, 120, 160, XXH
8" IPS 8.625" O.D. SCH 5, 10, 40, 80, 120, 160, XXH
10" IPS 10.750" O.D. SCH 10, 20, 40, 80 (5.00), TRUE 80(5.00)
12" IPS 12.750" O.D. SCH 10, 20, 40(375), TRUE40(406), SCH80(500)
14" IPS 14.000" O.D. SCH10 (188), SCH40 (375)
16" IPS 16.000" O.D. SCH10(188), SCH40(375)
18" IPS 18.000" O.D. SCH-40 (375)

 

Chemical Composition of Inconel 601 Pipes

Grade C Mn Si S Cu Fe Ni Cr
Inconel 601 0.10 max 1.0 max 0.5 max 0.015 max 1.0 max Balance 58.0–63.0 21.0–25.0

 

Mechanical Properties of B167 Inconel 601 Pipe

Element Density Melting Point Tensile Strength Yield Strength (0.2% Offset) Elongation
Inconel 601 8.1 g/cm³ 1411 °C (2571 °F) 80,000 psi (550 MPa) 30,000 psi (205 MPa) 30%

 

Physical Properties of Inconel 601 Pipes

Property Value
Density (lb / cu. in.) 0.293
Specific Gravity 8.11
Specific Heat (Btu/lb/°F [32–212°F]) 0.107
Electrical Resistivity (microhm-cm at 68°F) 710
Melting Point (°F) 2460
Thermal Conductivity 87
Mean Coefficient of Thermal Expansion 7.6
Magnetic Permeability 1.003
Modulus of Elasticity (Tension) 29.95 (×10⁶ psi)

 

Inconel 601 Pipe Pressure Rating

Tube O.D. (in.) Working Pressure (psig) per Wall Thickness (inches)
  0.028 in 0.035 in 0.049 in 0.065 in 0.083 in 0.095 in 0.109 in 0.120 in
1/8 7900 10100 - - - - - -
1/4 3700 4800 7000 9500 - - - -
5/16 - 3700 5400 7300 - - - -
3/8 - 3100 4400 6100 - - - -
1/2 - 2300 3200 4400 - - - -
3/4 - - 2200 3000 4000 4600 - -
1 - - - 2200 2900 3400 3900 4300

 

Inconel 601 Pipe Uses

There are many sectors and industries consuming ASTM B167 Inconel 601 Pipe like:

Industry / Application Description / Use Case
Manufacturing of conveyor shafts Heavy-duty material handling systems
Military & Defence industry Defence and strategic applications
Heavy engineering Industries Large-scale industrial machinery and components
Oil and Gas Industries Piping and equipment in corrosive and high-temperature environments
Agricultural sector Machinery and equipment used in farming and processing
Railway engines and coaches Components for locomotives and railway carriages
Manufacturing of arms and ammunition Defence and firearms industry
Manufacturing gears, bearings, and hinges Precision mechanical components
Aerospace High-temperature and corrosion-resistant aerospace components

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

Gnee Steel
 
 

About Gnee Steel

Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.

 
35000+

Square Meters Built

 
200+

Enterprise Employees

 
18+

Years Experience

 
160+

Partner countries

Send Inquiry

whatsapp

Phone

E-mail

Inquiry