Dec 03, 2025 Leave a message

Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Alloy 718 Flange: Properties, Dimensions and Welding Guidance

What Alloy 718 Flanges Are

Alloy 718 flanges (UNS N07718, W.Nr. 2.4668) are forged or machined nickel-chromium components used to join pipe, tube, valves and pressure equipment in high-temperature, high-stress service. The grade pairs corrosion resistance with an aged strength level that few austenitic stainless steels can approach, so a flanged joint that must hold sealing load at several hundred degrees can be built with a lighter section and a smaller bolt circle than an equivalent lower-strength material would allow.

Why Alloy 718 Is Selected for Flanged Joints

High tensile and yield strength after aging, with good toughness retained at low temperature

Creep and stress-rupture resistance at temperatures up to about 704 °C (1,300 °F)

Oxidation resistance at temperatures up to about 982 °C (1,800 °F)

Essentially non-magnetic, so it does not disturb instrumentation or magnetic-sensitive equipment

Good weldability in both the age hardened and the solution annealed condition

High reflectivity to laser radiation at shorter wavelengths, which must be considered when flanges are cut or profiled by laser

The most common type for critical high-temperature piping is the welding neck flange, because the tapered hub transfers flange load into the pipe wall gradually and keeps the joint concentric under thermal cycling. Blind, slip-on, socket weld, lap joint and threaded patterns are also produced from the same grade where the duty allows.

Chemical Composition of Alloy 718 Flanges

Element, wt% Alloy 718 (UNS N07718)
Nickel (Ni) 50.00–55.00
Chromium (Cr) 17.00–21.00
Iron (Fe) Balance
Molybdenum (Mo) 2.8–3.3
Niobium + Tantalum (Nb+Ta) 4.75–5.50
Aluminium (Al) 0.20–0.80
Titanium (Ti) 0.65–1.15
Carbon (C) 0.08 max
Manganese (Mn) 0.35 max
Silicon (Si) 0.35 max
Copper (Cu) 0.30 max
Sulfur (S) 0.015 max

Iron is the balance of the alloy, and the controlled titanium, aluminium and niobium levels are what allow the aging response that produces the flange's strength. Common product standards for the grade include ASTM B637 for bar and forging stock and AMS 5662 / AMS 5663 for heat-treated product, with flanges machined from material certified to those specifications.

Mechanical Properties and Weld Neck Dimensions

Property Solution treated / annealed Aged
Tensile strength 930 MPa (135,000 psi) 1,240–1,550 MPa
0.2% yield strength 482 MPa (70,000 psi) 760–1,310 MPa
Elongation in 50 mm 45% 12–30%
Hardness About 100 HRB 250–360 HB, about 22–35 HRC
Density 8.2 g/cm³ 8.2 g/cm³

Representative weld neck flange dimensions for common sizes are listed below. Bore dimensions follow the mating pipe schedule, and the raised face height of 2 mm and weld face of 1.6 mm are consistent across the range shown.

Nominal size DN Outer dia. (mm) Flange thk. (mm) Hub OD (mm) Weld neck OD (mm) Weld neck length (mm) Raised face dia. (mm) Bolt circle (mm)
1/2 in 15 90 9.6 30 21.3 46 34.9 60.3
3/4 in 20 100 11.2 38 26.7 51 42.9 69.9
1 in 25 110 12.7 49 33.4 54 50.8 79.4
1 1/2 in 40 125 15.9 65 48.3 60 73.0 98.4
2 in 50 150 17.5 78 60.3 62 92.1 120.7
3 in 80 190 22.3 108 88.9 68 127.0 152.4
4 in 100 230 22.3 135 114.3 75 157.2 190.5
6 in 150 280 23.9 192 168.3 87 215.9 241.3
8 in 200 345 27.0 246 219.1 100 269.9 298.5
10 in 250 405 28.6 305 273.0 100 323.8 362.0
12 in 300 485 30.2 365 323.8 113 381.0 431.8

Larger sizes, including 14 in through 24 in, are produced to the same dimensional pattern, with outer diameters rising to about 815 mm and thickness to about 46 mm. Final dimensions should always be confirmed against the piping class and the applicable dimensional standard before machining begins.

Welding, Magnetism and Service Limits

Alloy 718 flanges are readily welded compared with many other high-temperature alloys, and welding is possible in either the age hardened or the solution annealed condition. For pressure-containing or cyclic duty, a qualified procedure and post-weld heat treatment are recommended, because the precipitation reactions in the heat-affected zone influence both strength and resistance to strain-age cracking. Matching filler metal and controlled interpass temperature help keep the joint consistent with the parent flange.

The alloy is non-magnetic, with good corrosion and oxidation resistance, and it suits parts that must resist creep and stress rupture at temperatures up to about 704 °C (1,300 °F) together with oxidation resistance at temperatures up to about 982 °C (1,800 °F). Bolting should be selected for the same temperature class as the flange so that the joint does not lose preload before the gasket is compressed. Traceability matters on flanged joints: positive material identification, hardness checks and non-destructive examination of the weld end are the usual release tests.

Frequently Asked Questions

Q: What is an Alloy 718 flange used for?
It connects pipe, tube, valves and pressure equipment in high-temperature, high-stress service, and is common in aerospace, oil and gas, power generation and automotive applications.

Q: Can Alloy 718 flanges be welded?
Yes. The grade has good weldability compared with other high-temperature alloys and can be welded in the age hardened or solution annealed condition, with post-weld heat treatment for critical joints.

Q: Are Alloy 718 flanges magnetic?
No. Alloy 718 is essentially non-magnetic, which makes it suitable where magnetic interference with instrumentation must be avoided.

Q: What temperature can Alloy 718 flanges withstand?
Creep and stress-rupture resistance is useful to about 704 °C (1,300 °F), and oxidation resistance extends to about 982 °C (1,800 °F).

Q: Which standards apply to Alloy 718 flanges?
Flanges are machined from material certified to specification for the grade, such as ASTM B637 for bar and forging stock and AMS 5662 or AMS 5663 for heat-treated product.

Q: Why is a welding neck flange preferred in hot service?
The tapered hub distributes flange load into the pipe wall and keeps the joint concentric, which limits leakage risk when the line expands and contracts with temperature.

Q: What hardness should be expected?
In the solution treated condition the alloy is about 100 HRB, while the aged condition reaches roughly 250–360 HB, equivalent to about 22–35 HRC.