Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Advantages of Alloy 600 for High-Temperature and Corrosive Service

What Alloy 600 Is

Alloy 600 is an austenitic nickel-chromium-iron alloy, designated UNS N06600 and Werkstoff 2.4816, containing at least 72% nickel together with 14-17% chromium. It was introduced in the 1930s and quickly became a reference material wherever high temperature and severe corrosion occur together. The combination of a high nickel content and a chromium addition gives the alloy both oxidation resistance and resistance to chloride ion stress corrosion cracking, which stainless steels cannot match at elevated temperature.

The alloy is supplied as bar, sheet, plate, seamless tube and wire under ASTM B166, ASTM B167 and ASTM B168, and each product form has a corresponding ASME specification for pressure-retaining service. Because it is a solid-solution alloy with a stable austenitic structure, it can be cold formed, hot formed and welded by conventional methods without complex heat treatment.

Chemical Composition of Alloy 600

Typical composition limits are shown below in weight percent.

Element Ni Cr Fe C Mn Si S Cu
Alloy 600 (UNS N06600) 72.0 min 14.0-17.0 6.0-10.0 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max

The balance of the alloy is nickel plus incidental residuals. The 6-10% iron content keeps the alloy austenitic and improves forging behaviour, while chromium provides the protective oxide that forms in oxidising atmospheres.

Main Advantages of Alloy 600

Oxidation resistance in air up to about 1093 °C, with useful creep and rupture strength at high temperature.

Very high resistance to chloride ion stress corrosion cracking compared with austenitic stainless steel.

Corrosion resistance in organic and inorganic media, including alkaline solutions, and in reducing as well as oxidising conditions.

Service from cryogenic temperatures to roughly 1093 °C in oxidising atmospheres.

Non-magnetic austenitic structure that remains stable in service.

Excellent weldability and formability by standard shop processes, including gas tungsten arc and shielded metal arc welding.

Resistance to dry chlorine and hydrogen chloride at elevated temperature and to many nitriding and carburising furnace atmospheres.

Mechanical and Physical Properties

Property Typical value
Density 8.47 g/cm³
Melting range 1354-1413 °C
Tensile strength 550 MPa
Yield strength (0.2% offset) 240 MPa
Elongation 30%
Modulus of elasticity 207 GPa
Thermal expansion 13.3 µm/m·°C (20-100 °C)

Values are typical for annealed product; cold worked tube and bar are stronger with reduced elongation. Alloy 600 retains useful strength and ductility at temperatures where most stainless steels and low-alloy steels have already scaled or softened.

Typical Applications

Heat-treating retorts, muffle and box furnace components, wire belts and roller hearth fixtures.

Nuclear reactor internals, control rod drive mechanisms and steam generator tubing.

Chemical processing equipment such as bubble towers, tube sheets, evaporator tubes and reactors.

Nitriding containers and baskets where nitrogen is diffused into a surface at high temperature.

Pulp and paper plant equipment handling abietic acid and sodium sulfide flaking trays.

Electronics parts including springs, tube support members, cathode-ray tube spiders and thyratron grids.

Limitations and Selection Notes

Alloy 600 is not immune to every environment. It can suffer stress corrosion cracking in concentrated caustic alkalies at high temperature and in certain high-purity water conditions, so water chemistry control and suitable stress relief are important in nuclear and boiler service. Reducing sulphur-bearing atmospheres above about 600 °C can attack the alloy, and strength is lower than that of precipitation-hardening nickel alloys, so heavier sections may be needed. Machining is slow because the material work hardens readily, and cutting tools must be sharp with generous depth of cut.

Frequently Asked Questions

Q: What is Alloy 600 used for?
It is used for furnace fixtures, heat-treating retorts, nuclear components, chemical process equipment, nitriding baskets and high-temperature electronic parts.

Q: How does Alloy 600 resist high temperatures?
Its high nickel and chromium content forms a tenacious protective oxide film, so the alloy resists scaling in air up to about 1093 °C and keeps useful strength at those temperatures.

Q: Is Alloy 600 resistant to chloride stress corrosion cracking?
Yes, the high nickel level gives strong resistance to cracking caused by chloride ions, which is a common failure mode for austenitic stainless steels.

Q: Is Alloy 600 magnetic?
No, it has a stable austenitic structure and is essentially non-magnetic, which suits instruments and electrical components that must not disturb magnetic fields.

Q: Can Alloy 600 be welded?
Yes, it welds well by gas tungsten arc, gas metal arc and shielded metal arc processes using matching filler metal, without preheat and usually without post-weld heat treatment.

Q: What are the main weak points of Alloy 600?
The alloy can crack in hot concentrated caustic solutions or specific high-purity water environments, and it is weaker than precipitation-hardening grades, so environment and load data should be reviewed before selection.