Inconel 600 pipe fittings perform exceptionally well in harsh environments, thanks to their superior corrosion/oxidation resistance (especially in high-temperature, acidic, and chloride environments), high mechanical strength (able to withstand high pressure and stress), and wide temperature range (from cryogenic temperatures to 2000°F), effectively preventing cracking and maintaining structural integrity in chemical, power generation, and marine applications.
Is Inconel 600 a type of stainless steel?
Like 314 stainless steel, Inconel 600 is considered a heat-resistant alloy. Its chemical composition allows it to maintain good strength and toughness even when subjected to extreme temperatures. Inconel 600 not only possesses excellent heat resistance, but its chemical composition also enables it to effectively resist corrosion.

Gnee Steel maintains a large inventory and supplies Inconel 600 butt weld pipe fittings in various sizes. Due to their excellent resistance to seawater corrosion, low biofouling rate, and good machinability, these products are widely used in the marine industry. Inconel 600 butt weld pipe fittings are a high-temperature, corrosion-resistant nickel-chromium alloy commonly used in demanding industrial applications such as aerospace, chemical, and nuclear industries. Chinese Inconel pipe fitting manufacturers recommend the 600 grade alloy due to its numerous superior properties. This alloy possesses high tensile and yield strength, making it suitable for high-stress conditions. ASTM B366 UNS N06600 elbows offer corrosion resistance. Using these components can extend the lifespan of equipment.
Inconel 600 Buttweld Fittings Range
| Butt Weld Tube Fitting Specification | ASTM A403/ ASTM SA403, ASTM A815 / ASME SA815, ASTM A420 / ASME SA420, ASTM A234 / ASME SA234, ASTM A860 / ASME SA860, ASTM B366 / ASME SB366, DIN 2605 Part 1 / DIN 2605 Part 2, EN10253-2 / EN10253-4 TC1 and TC2 |
| Butt Weld Tube Fitting Manufacturing Process | Hot / Cold / Fabricate / Seamless / Welded / Induction |
| Butt Weld Tube Fitting Other Grades | Stainless Steel - 304, 304L, 304H, 310s, 316, 316L, 317L, 321, 347, 904L, 410, 446 etc. Duplex and Super Duplex - UNS N031803, UNS N032750, UNS N032760 etc. Inconel - 600, 601, 625, 718, UNS N06600, UNS N06601, UNS N06625, UNS N07718 etc. Incoloy - 800, 800H, 800HT, 825, UNS N08800, UNS N08810, UNS N08811, UNS N08825 etc. Monel - 400, UNS N04400 etc. Hastelloy - C276, C22, UNS N010276, UNS N06022 etc. Other - Alloy 20, SMO 254, UNS N08020, UNS N031254 etc. EN / DIN P235GHTC1/2 (St 35.8 I/ III), P265GH, S355J2H 16Mo3 (15Mo3), 10CrMo9-10 (10CrMo910), 13CrMo4-5 (13CrMo44) X11CrMo5, X11CrMo9-1, X20CrMOV11-1, X10CrMoVNb9-1, X10CrWMoVNb9-2, 7CrMoVTiB10-10 P215NL (TTST35N/V), 12Ni14 (10Ni14) P355N (StE355), P355NH (WStE355), P355NL1 (TStE355), P355NL2, L290NB (STE 290.7), L360NB (STE 360.7) 1.4301, 1.4306, 1.4362(Lean Duplex), 1.4401, 1.4404, 1.4435, 1.4436, 1.4439, 1.4462(Duplex), 1.4466(Super Duplex), 1.4501, 1.4539, 1.4541, 1.4550, 1.4571 1.4841, 1.4878,, 1.4876, 1.4952, 1.4835, 1.4877, 1.4910 |
| Butt Weld Fittings Outer Diameter | 1/2" NB TO 48" NB |
| Butt Weld Fittings Wall Thickness or Schedule | Sch 10s to Sch XXS or As Per Custom Requirement |
| Butt Weld Fittings Types | 45 Degree Elbow, 90 Degree Elbow, 180 Degree Elbow, LR Elbow (Long Radius Elbow), SR Elbow ( Short Radius Elbow), Equal Tee, Reducing / Unequal Tee, Concentric Reducer, Eccentric Reducer, End Cap, Long Stub End, Short Stub End, Lap Joint Stub End, Equal Cross, Reducing / Unequal Cross, Seamless Fittings, Welded Fittings, 1.5D, 3D, 5D etc. |
| Butt Weld Fittings Dimension | ASME 16.9 - Factory-Made Wrought Buttwelding Fittings ASME B16.28 - Wrought Stainless Steel Buttwelding Short Radius Elbow and Returns MSS SP-43 - Wrought and Fabricated Butt-Welding Fittings for Low Pressure, Corrosion Resistant Applications |
| Butt Weld Fittings Other Testing | Tensile, Hardness Test, Chemical Analysis – Spectro Analysis, Positive Material Identification – PMI Testing, Flattening Test, Micro and Macro Test, Pitting Resistance Test, Flaring Test, Intergranular Corrosion (IGC) Test, NACE MR0175, Ultrasound Test, ASTM A262 Practice E, Charpy Impact Test, Grain Size, Dye Penetrant Test etc. |
| Butt Weld Fittings Packaging | Carrate / Wooden Pallet / Wooden Box |
| Butt Weld Fittings Shipment & Transportation | By Road - Truck / Train Partial Load, Full Load, By Sea - Break-bulk Conventional Vessel / FCL (Full Container Load) / LCL (Less Container Load) / 20 Feet Container / 40 Feet Container / 45 Feet Container / High Cube Container / Open Top Container, By Air - Freighter Civil Passenger and Cargo Planes |
Inconel 600 butt weld pipe fittings and connectors
Seamless/welded, 100% radiographic testing
| Products | Size | |
| Inconel 600 Buttweld Fittings Elbow – Long Radius | Inconel 600 Buttweld Fittings Stub Ends | Sizes 1/2″ – 24″ |
| Inconel 600 Buttweld Fittings Elbow – Short Radius | Inconel 600 Buttweld Fittings Cross | |
| Inconel 600 Buttweld Fittings Reducing Elbow | Inconel 600 Buttweld Fittings Reducing Cross | |
| Inconel 600 Buttweld Fittings 45° Elbow | Inconel 600 Buttweld Fittings Tees | |
| Inconel 600 Buttweld Fittings Fabricated Tee | Inconel 600 Buttweld Fittings End Cap | |
| Inconel 600 Buttweld Fittings Reducer | Inconel 600 Buttweld Fittings Seamless Fittings | |
| Inconel 600 Buttweld Fittings Concentric Reducer | Inconel 600 Buttweld Fittings Pipe Nipple | |
| Inconel 600 Buttweld Fittings Eccentric Reducer | Inconel 600 Buttweld Fittings 5D Elbow | |
| Inconel 600 Buttweld Fittings 3D Elbow | Inconel 600 Buttweld Fittings Welded Pipe Fitting | |
Types Of Grade Inconel 600 Pipe Fitting





Reducer

Reducer



Cap


Cross

Tee
Chemical Composition of Inconel 600 Pipe Fitting
| Grade | C | Mn | Si | S | Cu | Fe | Ni | Cr |
| Inconel 600 | 0.15 max | 1.00 max | 0.50 max | 0.015max | 0.50 max | 6.00 – 10.00 | 72.00 min | 14.00 – 17.00 |
Mechanical Properties of Inconel 600 Buttweld Fittings
| Element | Density | Melting Point | Tensile Strength | Yield Strength (0.2%Offset) | Elongation |
| Inconel 600 | 8.47 g/cm3 | 1413 °C (2580 °F) | Psi – 95,000 , MPa – 655 | Psi – 45,000 , MPa – 310 | 40 % |
Equivalent Grade of Inconel 600 Pipe Fitting
| STANDARD | WERKSTOFF NR. | UNS | JIS | BS | GOST | AFNOR | EN |
| Inconel 600 | 2.4816 | N06600 | NCF 600 | NA 13 | МНЖМц 28-2,5-1,5 | NC15FE11M | NiCr15Fe |
Other Available Products Of Inconel 600 Pipe Fitting
| Inconel 600 Pipe Tube Fitting | Inconel 600 Buttweld Pipe Fittings |
| Inconel 600 Seamless Pipe Fittings | Inconel 600 Welded Pipe Fittings |
| Inconel B366 600 Pipe Elbow | Inconel Alloy 600 Buttweld Tee |
| Inconel 600 Buttweld Reducer Suppliers | ANSI 600 Inconel Pipe Fittings |
| Inconel UNS N06600 Stubends Dealer | ASTM B366 Inconel Pipe Fittings Exporter |
| Inconel Alloy Butt weld Fittings Stockholder | Inconel UNS N06600 Pipe End Cap Distributors |
| Inconel 600 45deg.Elbow | B366 Inconel 90deg. LR Elbow Manufacturer |
Test Certificates
We provide Inconel 600 pipe fittings that meet the following requirements: factory test certificates conforming to EN 10204 3.1 standard, PMI testing, test reports from NABL accredited laboratories, 3.2 certification from a third-party external inspection agency, ultrasonic testing reports, and X-ray testing reports.
Why Choose Gnee as Your Nickel-Based Alloy Supplier
✅ Over 18 years of export experience, products sold to more than 80 countries
✅ Certified by ISO, SGS, and BV
✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars
✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging
✅ Fast delivery within 7-15 days, supported by global logistics partners
📦 Packaging and Shipping
All stainless steel products are packaged using the following methods:
Wooden pallets or crates
Moisture-proof packaging
Labels with furnace number, standard, and size labels
Shipped worldwide by sea, air, or express
Marking and Packaging
Our Inconel 600 pipes are specially packaged to ensure they are not damaged during transportation. For export, the standard export packaging is wooden crates. All Inconel 600 pipes are marked with our grade, batch number, size, and markings. We can also provide customized branding on the products according to the buyer's specific requirements. If you have any specific requirements regarding packaging or dimensions, please contact us for a quotation at ss@gneesteel.com