The king of deformed high temperature alloy GH4169
GH4169, also known as Inconel 718, is a precipitation-strengthened nickel-based high-temperature and high-strength alloy. Inconel 718 has good comprehensive properties in the temperature range of -253~700℃. The yield strength below 650℃ ranks first among deformed superalloys. It also has good fatigue resistance, radiation resistance, oxidation resistance, corrosion resistance, and good With its processing performance, welding performance and long-term structural stability, it can manufacture various parts with complex shapes. It has been widely used in the aerospace, nuclear energy, and petroleum industries within the above temperature range.
Another feature of this alloy is that the alloy's structure is particularly sensitive to the thermal processing process. By mastering the phase precipitation and dissolution rules in the alloy and the relationship between the structure, process, and properties, reasonable and feasible process procedures can be formulated for different use requirements. A variety of parts are available to meet different strength levels and usage requirements.


Inconel 718 has the following features:
1.Easy processability
2. It has high tensile strength, fatigue strength, creep resistance and fracture strength at 700℃
3. High oxidation resistance at 1000℃
4. Stable chemical properties at low temperatures
5.Good welding performance
The metallographic structure of Inconel 718, 718 alloy has an austenitic structure. The γ" phase generated after precipitation hardening gives it excellent mechanical properties. The δ phase generated at the grain boundary during the heat treatment process gives it the best mechanical properties. of plasticity.
Corrosion resistance of Inconel 718: No matter in high or low temperature environments, 718 alloy has excellent resistance to stress corrosion cracking and pitting corrosion. Alloy 718 has particularly excellent oxidation resistance at high temperatures.
Inconel 718 process performance and requirements: (1) Thermal processing: The suitable thermal processing temperature is 1120-900°C. The cooling method can be water quenching or other rapid cooling methods. After thermal processing, it should be annealed in time to ensure the best performance. During thermal processing, the material should be heated to the upper limit of the processing temperature. In order to ensure the plasticity during processing, the final processing temperature when the deformation reaches 20% should not be lower than 960°C. (2) Cold working: Cold working should be carried out after solid solution treatment. The work hardening rate is greater than austenitic stainless steel, so the processing equipment should be adjusted accordingly, and there should be an intermediate annealing process during the cold working process.
Inconel718 welding process: The alloy has satisfactory welding performance and can be welded by argon arc welding, electron beam welding, seam welding, spot welding and other methods.
Inconel718 parts heat treatment process: The heat treatment of aviation parts is usually carried out according to the standard heat treatment system and the direct aging heat treatment system.
Application scope of Inconel 718: Due to its high temperature strength at 700°C, excellent corrosion resistance and easy processability, 718 can be widely used in various high-demand situations.
1.Steam turbine
2. Liquid fuel rocket
3.Cryogenic engineering
4.Acidic environment
5. Nuclear Engineering