Datasheet-For-Inconel-600-1-7-(1)-1-6.pdf

Performance advantages of Inconel 600 round bar

 
Inconel 600 round bar
Performance advantages of Inconel 600 round bar
01

Performance advantages of Inconel 600 round bar

Inconel 600 round bar offers significant performance advantages, including excellent resistance to heat, oxidation, and corrosion, making it particularly suitable for use in high-temperature and aggressive chemical environments. It maintains strength from cryogenic to elevated temperatures and resists stress corrosion cracking in chloride-free solutions, making it suitable for use in the aerospace, petrochemical, and power generation industries.

02

What is the Rockwell hardness of Inconel 600?

Inconel 600 has a Rockwell hardness range of 65B to a maximum of 84B. This gives the grade excellent strength, ductility, and enhanced wear resistance in stress-inducing environments.

Inconel 600
 
 

Inconel 600 Bars Specification

SpecificationsASTM B166 / ASME SB166

StandardASTM, ASME and API

Range5 mm to 500 mm Dia

Length100 mm to 6000 mm

FinishingBright, Polish & Black

FormRound, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wire-mesh, Billet, Ingot, Forging Etc.

Grade 600 UNS (N06600), DIN (2.4816)

Inconel 600 Round Bar Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

Inconel 600 Round Bars Mechanical Properties

Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
8.47 g/cm3 1413 °C (2580 °F) 655 MPa, 95000 psi 310 MPa, 45000 psi 45 %

Advantages of Inconel 600 Round Bar
Inconel 600 round bar is versatile and offers excellent resistance to oxidation and corrosion. Due to its high nickel content, the alloy is resistant to various corrosion processes, including stress corrosion cracking, pitting, crevice corrosion, and intergranular corrosion. These bars also exhibit high strength at high temperatures.

Inconel 600 round bar is widely used in various industries, including shipbuilding and heavy engineering, oil and gas, pulp and paper, pharmaceuticals, aerospace, and chemicals.

Forged from a nickel-chromium alloy, Inconel 600 round bar offers high-temperature resistance, making it an ideal choice for many industries. It also offers strong corrosion resistance, making it a preferred choice for many applications.

Inconel 600 round bar is able to withstand high temperatures and corrosive environments. This makes it an ideal choice for gas turbine blades and exhaust nozzles, as it can withstand high temperatures while maintaining structural integrity. Additionally, some Inconel alloys are used in marine applications, where their excellent saltwater and corrosion resistance make them ideal for such environments.

This alloy is resistant to chlorides and carburization and is non-magnetic. Inconel 600 is also resistant to chlorides and oxidizing environments. It also has a high nickel content, making it ideal for high-temperature applications. This alloy is very strong and durable, with excellent mechanical properties.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.