Is nickel an Inconel?
What is Inconel?
Inconel is a family of nickel-chromium-based high-temperature alloys that are used in a wide range of applications. Inconel is considered to have excellent resistance to oxidation and corrosion, and high performance at high temperatures. Inconel alloys also offer an excellent combination of toughness and strength for demanding applications or harsh environments subject to pressure and heat.
When heated, Inconel forms a thick, stable oxide layer that protects the surface of the material from further attack. Its excellent high-temperature strength comes from solid solution strengthening or precipitation hardening, depending on the alloy. Inconel differs from Incoloyâ in composition and purpose. Inconel performs better than Incoloy in demanding, high-temperature applications - although Inconel is more difficult to manufacture than Inconel.


Key advantages of Inconel alloys include:
Good resistance to acids (sulfuric, phosphoric, nitric, and hydrochloric acids)
Almost no chloride-induced stress corrosion cracking
Excellent mechanical properties at all temperatures
Excellent resistance to pitting, crevice, and intergranular corrosion
High oxidation resistance at high temperatures
There are several types of Inconel alloys, each with its own composition. Inconel alloys have specific properties that make them effective in different situations. For example, Inconel 600 is often used in chemical and food processing equipment because of its corrosion and oxidation resistance. On the other hand, Inconel 625 is often used in aerospace and marine engineering applications because of its high strength and the fact that it does not require heat treatment.
Typical Applications and Uses of Inconel Alloy
Inconel alloy is well suited for a variety of industrial applications, including aircraft, marine, chemical processing, power generation, nuclear energy, gas turbines, aerospace, and automotive. Typical uses for Inconel are turbine blades and seals, submersible well pump motor shafts, and high-temperature fasteners on specialized machinery. Other uses include chemical processing and heat exchange tubes, steam generators, pollution control equipment, and critical core components in nuclear pressurized water reactors.
Is Inconel Considered Steel?
Inconel is not considered steel or stainless steel. While both stainless steel and Inconel have a silver finish and use a numbering system for alloys and strengths, they differ in quality, properties, uses, and weight.
With its nickel, chromium, and molybdenum composition, Inconel is corrosion and pitting resistant and is available in several different alloys. Costing more than stainless steel, the surface of Inconel can be textured for a matte finish or smoothed for a bright finish.
Stainless steel has carbon, manganese, phosphorus, sulfur, silicon, chromium, and nickel as its composition; as well as a protective oxide layer that can be damaged by continued exposure to extreme conditions. Stainless steel comes in a number of different grades.
Stainless steel is also heavier than Inconel alloys. For example, Inconel jewelry looks like stainless steel but the weight feels a lot like aluminum. Stainless steel is also not as heat resistant as Inconel. This makes Inconel more suitable for certain industrial products than stainless steel.
Forged Inconel Alloys
Inconel is widely used in the forging industry to produce high-quality, oxidation-resistant end products. This is because corrosion is one of the most common problems in industries that use forged materials. Manufacturers have tried using Inconel in a variety of applications and found it to be both practical and useful, so they continue to use it.
Forging presses metals under tremendous pressure into high-tensile-strength components. This manufacturing process improves the grain structure and improves the metal's physical properties (ductility, toughness, and strength) so that grain flow can be oriented along the principal stress directions encountered in actual use.
The key advantages of forging are:
Better than casting or machined bar stock
Stronger parts than other metalworking processes
Highly formable into almost any product
Versatile and can be used in any industry
Cost-effective for high-volume manufacturing
Machining Inconel
Machining Inconel requires high cutting forces and highly developed skills to ensure the process is done correctly in a consistent, repeatable manner. To work with Inconel properly, one needs to understand its characteristics and how to compensate for its limitations. Machining tips include:
Always check tools for signs of wear
Start with solution metal
Use ceramic cutting tools for continuous cuts
Avoid pecking when drilling Inconel
Use end mills with more flutes
Use drills with replaceable tips
Use cobalt roughing cutters
Consider rigidity – fixtures, machine tools
These are just a few of the machining tips that fabricators should know when working with high nickel alloys like Inconel.