Jan 29, 2024 Leave a message

Inconel718 Ingredient|Performance|Technology|Application

Inconel718 Ingredient|Performance|Technology|Application

 

Inconel 718 (GH4169)
Overview:
The commonly used 718 alloy can be divided into two categories according to strength, 718 according to the AMS specification, with a yield strength of 150ksi, and 718 according to the NACE specification, with a yield strength of 120ksi.
Alloy 718 is a precipitation hardenable nickel-based alloy that exhibits high yield strength, tensile strength and creep cracking strength in high temperature environments up to 704°C. The age hardening reaction of alloy 718 is relatively slow, so it does not harden with heating and cooling during annealing and welding. Compared with other nickel-based super alloys with added aluminum and titanium, alloy 718 has excellent welding properties.
Similar brands:
GH4169, GH169 (China),
NC19FeNb (France),
NiCr19Fe19Nb5, Mo3 (Germany),
NA 51 (UK)
Inconel718,UNS NO7718(USA)
NiCr19Nb5Mo3(ISO)
chemical composition:
C≤0.08
Mn≤0.35
Si≤0.015
P≤0.35
S≤0.015
Cr17~21
Ni50~55
Mo2.8~3.3
Cu≤0.3
Ti0.65~1.15
Al0.2~0.8
Fe margin
Nb4.75~5.5
B≤0.006

Inconel718 Ingredient|Performance|Technology|Application

Inconel718 Ingredient|Performance|Technology|Application

Physical properties:
Density ρ=8.24g/cm3
Melting temperature range 1260~1320℃

Mechanical behavior:
Tensile strength: 150ksi and above
Yield Strength: 120-145ksi
4D elongation: more than 20%
Area shrinkage (dia≤10"): more than 35%
Area shrinkage (dia>10"): more than 25%
Hardness: 30-40HRC
V-notch impact strength (-59°C or lower):
Average energy: 35ft/lbs (47J) or more
Minimum energy per time: 30ft/lbs (40J)

heat treatment
Solution annealing at 1021-1052°C for 1-2.5 hours, then water quenching. Bars with a diameter less than 3.5" can be water quenched or air cooled. Aged at 774-802°C for 6-8 hours, then air cooled.
Heat treatment needs to be carried out by the steel factory, or under the guidance of the steel factory.
application
Jet engine and high-speed airframe parts such as wheels, turbine blades, gaskets, high-temperature bolts, fasteners, etc.

heat treatment

Method 1: Get the best tensile strength and stress cracking strength

954-982°C, 1 hour, air cooling +718°C, 8 hours, cool to 621°C at 56°C/hour, keep warm for 8 hours, then air cool.

Method 2: Obtain the best room temperature and low temperature tensile strength

Heat treatment at 1066°C for 1-2 hours, air cooling at +718°C for 8 hours, cooling to 621°C at 56°C/hour, heat preservation for 8 hours, and then air cooling.

Processing performance

Thermal processing

The furnace temperature for thermal processing does not exceed 1121°C. If the working temperature is below 593°C, the temperature range of cold working is controlled at 927-1010°C, which can provide forging strength. Avoid prolonged heating in the furnace when forging.

Machine processing

Both annealed and age-hardened states can be machined. The age-hardened state makes it easier to break and cut, and the surface finish is better. For annealed materials, machined tool life is slightly longer.

welding

Both the annealed state and the aged state of 718 can be welded. When welding aged materials, deformation will occur in the area where the weld is heated and softened.

 