Dec 05, 2025 Leave a message

Datasheet-For-Inconel-601-1-6-(1)-(1).pdf

Inconel Alloy 600 VS Inconel Alloy 601: the Key Differences You Should Know

 
 
 
Inconel Alloy 600 VS Inconel Alloy 601: the Key Differences You Should Know
Inconel Alloy 600 VS Inconel Alloy 601 the Key Differences You Should Know
01.

Inconel Alloy 600 VS Inconel Alloy 601: the Key Differences You Should Know

Inconel 600 vs. 601: The main differences lie in their composition and performance. Inconel 601 contains added aluminum (Al), resulting in superior high-temperature oxidation/carburization resistance and creep strength; while Inconel 600 has a higher nickel (Ni) content, making it suitable for general high-temperature/corrosive environments, but its stability at extreme temperatures is not as good as 601. For furnace components, heat exchangers, and aerospace applications, 601 is recommended; for chemical processing, refining, and general furnace applications (where extreme oxidation is not a primary consideration), 600 is recommended.

02.

What are the applications of Inconel 601 alloy?

In industrial furnaces, this alloy is used to manufacture radiant tubes, furnace chambers, rotary kilns, flame shields, annealing tubes, woven conveyor belts, chain curtains, burner nozzles, and resistance heating elements.

Inconel 601 Alloy

What is Inconel 600?

Inconel 600 is a nickel-chromium alloy renowned for its excellent oxidation resistance, corrosion resistance, and high-temperature performance. It maintains its strength and stability over a wide temperature range, making it ideal for applications such as chemical processing, aerospace, and nuclear reactors.

 

What is Inconel 601?

Inconel 601 is a nickel-chromium alloy with a higher aluminum content, exhibiting superior resistance to oxidation and high-temperature scaling. Its excellent durability makes it suitable for heat treatment equipment, furnace components, and combustion systems.

 

Chemical composition comparison of Inconel Alloy 600 and 601

Element Inconel 600 Inconel 601
Nickel (Ni) 72% 58-63%
Chromium (Cr) 14-17% 21-25%
Iron (Fe) 6-10% Balance
Aluminum (Al) - 1.0-1.7%
Carbon (C) ≤ 0.15% ≤ 0.10%
Manganese (Mn) ≤ 1.0% ≤ 1.0%
Silicon (Si) ≤ 0.5% ≤ 0.5%

 

Comparison of corrosion resistance of Inconel 600 and Inconel 601 alloys

Corrosive Environment Inconel 600 Inconel 601
Oxidation Excellent up to 1093°C Superior up to 1260°C
Sulfuric Acid Good Moderate
Hydrochloric Acid Limited resistance Limited resistance
High-Temperature Gases Excellent Excellent
Aqueous Corrosion Good in alkaline solutions, less effective in acidic environments Good but more suited to high-temperature corrosion

 

Comparison of Physical Properties of Inconel 600 and Inconel 601 Alloys

Property Inconel 600 Inconel 601
Density 8.47 g/cm³ 8.11 g/cm³
Melting Point 1354-1413°C 1365-1410°C
Thermal Conductivity 14.9 W/m·K at 20°C 13.3 W/m·K at 20°C
Tensile Strength 550 MPa 655 MPa
Yield Strength 240 MPa 310 MPa
Elongation 30% 33%

 

Comparison of Mechanical Properties of Inconel 600 and Inconel 601 Alloys

Property Inconel 600 Inconel 601
Tensile Strength 550 MPa 655 MPa
Yield Strength 240 MPa 310 MPa
Hardness (Rockwell B) 88 95
Elongation at Break 30% 33%
Creep Resistance Good Excellent

 

Comparison of Thermal Properties of Inconel 600 and Inconel 601 Alloys

Property Inconel 600 Inconel 601
Melting Point 1354-1413°C 1365-1410°C
Maximum Service Temperature 1093°C 1260°C
Thermal Conductivity 14.9 W/m·K at 20°C 13.3 W/m·K at 20°C
Thermal Expansion 13.3 µm/m·°C at 20°C 12.9 µm/m·°C at 20°C

 

Applications

Application Area Inconel 600 Inconel 601
Chemical Processing Heat exchangers, evaporator tubes, reactor vessels Furnace liners, catalyst support grids
Aerospace Jet engine components, turbine blades Combustion chambers, exhaust systems
Nuclear Industry Reactor control rods, heat shields Heat-treating baskets, nuclear reactor internals
Power Generation Steam generators, boiler components Heat recovery systems, gas turbine components
Petrochemical Industry Ethylene production, petrochemical heaters Radiant tubes, thermal reactors
Heat Treatment Annealing and carburizing equipment Furnace muffles, retorts, radiant tubes

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 600 alloy, offering a wide range of products including: seamless pipe (sizes: 4-219 mm; thickness: 0.5-20 mm); welded pipe (sizes: 5.0-1219.2 mm; thickness: 0.5-20 mm); plates (thickness: 0.1 to 100 mm; width: 10-2500 mm); strips; alloy round bars (diameter: 3-800 mm); flat bars (thickness: 2-100 mm; width: 10-500 mm); hexagonal bars (size: 2-100 mm); wire rods; and extruded profiles. We collaborate with steel mills to provide our customers with Inconel 600 alloy products that meet or exceed numerous leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN, and BS standards.


Gnee Steel stocks and sells Inconel 600, pipes, plates, strips, round bars, flat bars, forged billets, hexagonal steel, wire rods, and extruded profiles. Please feel free to contact us at ss@gneesteel.com for a quote.

Gnee Steel

Send Inquiry

whatsapp

Phone

E-mail

Inquiry