Jan 27, 2026 Leave a message

Inconel 718 vs 825 Round Bars

Gnee Steel is a leading manufacturer, exporter, and importer of Inconel 718/825 round bars. These products are highly sought after across various industries. Made from Inconel stainless steel, these round bars offer superior performance, including both seamless and welded tubing, and feature extremely high melting points.

Gnee Steel supplies Inconel 718/825 round bars at the most competitive prices. We manufacture these products strictly according to international and national standards, consistently ensuring the use of high-quality materials and rigorously testing all production materials.

 
Inconel 718 vs 825 Round Bars

Inconel 718 vs 825 Round Bars

 

Inconel 718 round bars offer exceptional high-temperature strength and fatigue resistance (up to 700°C), making them ideal for aerospace and turbine applications. Incoloy 825 bars (often simply referred to as 825) offer superior resistance to acid corrosion and chloride stress cracking, making them ideal for the chemical and oil and gas industries. Inconel 718 round bars are precipitation hardened, resulting in high strength (tensile strength 130-220 ksi), while alloy 825 bars are typically used in the annealed state, resulting in lower strength.

Is Inconel 825 magnetic?

 

The primary factors determining the applications of this alloy are its strength and heat resistance, not its magnetism. - Inconel 825: Inconel 825 contains iron, but in a lower amount than Inconel 600. Like other high-nickel alloys, it is generally considered non-magnetic.

Inconel 825

Inconel 718 round bars offer greater flexibility and strength than other alloy grades. They are hardened through high-temperature quenching. They exhibit excellent weldability and superior resistance to fracture and creep, contributing to the alloy's strength and durability. Inconel 718 round bars remain stable at both high and low temperatures. These Inconel 718 round bars possess exceptional resistance to oxidation, corrosion, and stress cracking. These seamless and welded tubings have a tensile strength of 130,000 psi and a yield strength of 75,000 psi.

 

Similarly, Inconel 825 round bars offer excellent corrosion resistance and are widely used in large-scale industrial applications such as petrochemicals, power generation, aerospace, and oil and gas. These round bars are commonly used in the manufacture of various equipment. These round bars offer interchangeable properties. The alloy has a tensile strength of 80,000 psi and a yield strength of 32,000 psi. The estimated suitable temperature for these bars is 1020°C.

 

Specification of Inconel 718/ 825 Round Bars

Specifications : ASTM B166 / ASTM SB166

Dimensions : ASTM, ASME and API

Size : 10 mm To 100 mm Dia in 100 mm TO 7180 mm Length.

Length : 3 to 6 meter, Custom Cut Lengths

Finish : Black, Bright Polished, Rough Turned, NO.4 Finish, Matt Finish, BA Finish

Form : Round, Square, Hex (A/F), Rectangle, Wire (Coil Form), Wiremesh, Billet, Ingot, Forging Etc.,

Condition : Cold Drawn & Polished Cold Drawn, Centreless Ground & Polished

 

Available Types of Inconel 718/ 825 Round Bars

Inconel 718/ Incoloy 825 Round Bars

Inconel 718/ Incoloy 825 Round Bars

Inconel 718/Incoloy 825 Hex Bars

Inconel 718/Incoloy 825 Hex Bars

Inconel 718/ Incoloy 825 Flat Bars

Inconel 718/ Incoloy 825 Flat Bars

Inconel 718/ Incoloy 825 Square Bars

Inconel 718/ Incoloy 825 Square Bars

Inconel 718/ Incoloy 825 Rectangular Bars

Inconel 718/ Incoloy 825 Rectangular Bars

Inconel 718/ Incoloy 825 Bright Bars

Inconel 718/ Incoloy 825 Bright Bars

 

Equivalent Grades of Inconel 718/ 825 Round Bars & Rods

STANDARD WERKSTOFF NR. UNS JIS BS GOST AFNOR EN
Inconel 718 2.4668 N07718 - - - - -
Incoloy 825 2.4858 N08825 NCF 825 NA 16 ЭП703 NFE30C20DUM NiCr21Mo

 

Chemical Composition of Inconel 718/ 825 Round Bars / Rods

Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015 max 0.30 max - 50.00 - 55.00 17.00 - 21.00
825 0.05 max 1.00 max 0.5 max 0.03 max 1.50 – 3.00 22.00 min 38.00 – 46.00 19.50 – 23.50

 

Inconel 718/ 825 Round Bars, Rods Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 718 8.2 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45 %
825 8.14 g/cm3 1400 °C (2550 °F) Psi – 80,000 , MPa – 550 Psi – 32,000 , MPa – 220 30 %

 

Why Choose Gnee as Your Nickel-Based Alloy Supplier

✅ Over 18 years of export experience, products sold to more than 80 countries

✅ Certified by ISO, SGS, and BV

✅ Global inventory of Inconel, Hastelloy, Incoloy, and Monel alloy tubing, plates, and bars

✅ Custom processing services available – including cutting, polishing, CNC machining, and packaging

✅ Fast delivery within 7-15 days, supported by global logistics partners

📦 Packaging and Shipping

All stainless steel products are packaged using the following methods:

Wooden pallets or crates

Moisture-proof packaging

Labels with furnace number, standard, and size labels

Shipped worldwide by sea, air, or express

Gnee Steel
 
 

About Gnee Steel

Gnee Steel is a professional manufacturer of nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy 800, Incoloy 800H/HT, Incoloy 825, Monel 400, Monel K500, and other high-temperature alloy materials. We specialize in the production and sales of alloy materials. Gnee Steel's products are widely used in aerospace, chemical, power generation, automotive, nuclear energy, and other fields, and we can provide customized alloy material solutions according to customer needs. For inquiries about alloy material prices or customized alloy material solutions, please feel free to contact us via email at ss@gneemetal.com for a quote.

 
35000+

Square Meters Built

 
200+

Enterprise Employees

 
18+

Years Experience

 
160+

Partner countries

Send Inquiry

whatsapp

Phone

E-mail

Inquiry