Aug 22, 2025 Leave a message

Inconel 718 Seamless Pipe Information

 
Inconel 718 Seamless Pipe
 
Inconel 718 Seamless Pipe Information

Inconel 718 Seamless Pipe Information

Inconel 718 tubing (UNS N07718) is a nickel-chromium high-temperature alloy known for its exceptional strength and high-temperature corrosion resistance. This seamless tubing is widely used in demanding industries such as aerospace (gas turbines, aircraft engines) and power generation, thanks to its high tensile strength and creep-rupture properties up to 700°C (1300°F), excellent weldability, and resistance to various cracking conditions. The alloy's precipitation-hardening properties allow it to be annealed and welded, and it does not autogenously harden.

What are the properties of Inconel 718 alloy?

Inconel 718 is a high-strength, corrosion-resistant nickel-based superalloy. It offers excellent mechanical properties, high-temperature strength, and resistance to oxidation and corrosion. Inconel 718 alloy is widely used in a variety of industries, including aerospace, oil and gas, automotive, and power generation.

Inconel 718 Alloy
 
Inconel 718 Alloy Tube Chemical Composition
Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015max 0.30 max – 50.00 – 55.00 17.00 – 21.00

718 Inconel Tubing Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 718 8.2 g/cm3 1350 °C (2460 °F) Psi – 1,35,000 , MPa – 930 Psi – 75,000 , MPa – 482 45 %

Inconel 718 Pipe Sizes

Wall Sizes ( O.D.)
.010 1/16" , 1/8" , 3/16"
.020 1/16" , 1/8" , 3/16" , 1/4" , 5/16" , 3/8"
.012 1/8"
.016 1/8" , 3/16"
.028 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 3/4" , 1" , 1 1/2" , 2"
.035 1/8" , 3/16" , 1/4" , 5/16" , 3/8" , 7/16" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.049 3/16" , 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/8" , 1 1/4" , 1 1/2" , 1 5/8" , 2" , 2 1/4"
.065 1/4" , 5/16" , 3/8" , 1/2" , 16" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 3/4" , 2" , 2 1/2" , 3"
.083 1/4" , 3/8" , 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 1 5/8" , 1 7/8" , 2" , 2 1/2" ,3"
.095 1/2" , 5/8" , 1" , 1 1/4" , 1 1/2" , 2"
.109 1/2" , 3/4" , 1" , 1 1/4" , 1 1/2" , 2"
.120 1/2" , 5/8" , 3/4" , 7/8" , 1" , 1 1/4" , 1 1/2" , 2" , 2 1/4" , 2 1/2" , 3"
.125 3/4" , 1" , 1 1/4" , 1 1/2" , 2" , 3" , 3 1/4"
.134 1"
.250 3"
.375 3 1/2"

Key Features of Inconel 718 Tubing
High-Temperature Strength: Inconel 718 Tubing maintains excellent yield strength, tensile strength, and creep-rupture strength at temperatures up to 700°C (1300°F).
Corrosion Resistance: It offers excellent resistance to oxidation, pitting, crevice corrosion, and stress corrosion cracking.
Weldability: Compared to other nickel-based superalloys hardened with aluminum and titanium, Inconel 718 Tubing offers superior weldability and resistance to strain-age cracking.
Hardness and Formability: The alloy achieves high strength through precipitation hardening while maintaining good formability and weldability in the solution annealed condition. 

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us at ss@gneesteel.com for a quote.