Inconel 718 plate is a high-temperature alloy that combines high strength, corrosion resistance, and excellent weldability. This nickel-based alloy contains significant amounts of niobium, iron, and molybdenum, along with smaller amounts of aluminum and titanium. Inconel 718 plate is used in aircraft engines and high-speed aircraft fuselage components, such as rudders, loads, and inserts, as well as high-temperature bolts and fasteners. Inconel 718 plate is also used in the oil and gas drilling and fabrication industries due to its high strength and resistance to chloride, pressure corrosion, and sulfide stress cracking.

What are the three main properties of Inconel 718?

 

Inconel 718 is a precipitation-hardening nickel-chromium alloy containing significant amounts of iron, niobium, and molybdenum, along with smaller amounts of aluminum and titanium. It combines corrosion resistance with high strength and excellent weldability, including resistance to post-weld cracking.

Inconel 718

Inconel 718 plate Specification

Inconel alloy 718 Plate Thickness 0.3 to 1200 mm or as required
Process of ASTM B166 UNS N07718 Plate Hot/ Cold Rolled
Available Length of Inconel 718 Plate 0-12mm or as required
Width of Nickel Alloy 718 Plate 0-2500mm or as required
Inconel 718 ASTM B166 Plate Surface No.1, No. 2D, No. 2B, BA, No.3, No.4, No.6, No.7, 2B, 2D, BA NO(8), Cold rolled sheet (CR), Hot rolled plate (HR), SATIN (Met with Plastic Coated), No.1 finish hot rolled Inconel 718 Plate, 1D, 2B, No.4, BA, 8K, satin, hairline, brush, mirror etc.

Chemical Composition of ASTM B670 Alloy 718 Plate


Ni
Cr Fe Mo Nb+Ta C Mn Si Ph S Ti Cu B Al Co
Min 50 17 Bal 2.8 4.75 - - - - - 0.65 - - 0.20 -
Max 55 21 - 3.3 5.50 0.08 0.035 0.35 0.015 0.015 1.15 0.30 0.006 0.80 1.00

Alloy 718 Plate Mechanical Properties in annealed condition


0.2% Proof Stress
Tensile Strength Elongation  
  MPA MPA %
  Max Max Min
Sheet and strip 550 965 30
Plate 725 1035 30

718 Alloy Plate Characteristics
Resistant to aqueous corrosion and chloride stress corrosion cracking
Extremely high yield strength, creep strength, and rupture strength
Good mechanical properties-tensile strength, fatigue strength, and creep rupture strength
Excellent weldability and resistance to post-weld aging cracking
Highly resistant to chloride and sulfide stress corrosion cracking
Age-hardenable, with a unique slow aging response that allows heating and cooling during annealing without risk of cracking.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.