Jul 17, 2025 Leave a message

Inconel 718 Alloy Flange

 
Inconel 718 Alloy Flange

Inconel 718 Alloy Flange

Inconel 718 flanges are metal components used to connect pipes or valves in high temperature and high stress applications. They are made of Inconel 718, a nickel-chromium alloy that has excellent corrosion resistance and high strength at high temperatures.

What are Inconel 718 flanges used for?

Inconel 718 alloy flanges are widely used in a variety of industries including aerospace, oil and gas, automotive, and power generation. 718 flanges have a high reflectivity to laser radiation, especially at shorter wavelengths. Reflectivity affects energy absorption and heat generation during laser processing.

Inconel 718 Alloy Flange
Inconel 718 Flanges

Can you weld Inconel 718 flanges?

Compared to other grades of high temperature alloys, Inconel 718 alloy flanges have good weldability. It can be welded in either the age hardened or solution annealed condition.

Are Inconel 718 alloy flanges magnetic?

Inconel 718 alloy flanges are non-magnetic. They have good corrosion and oxidation resistance and are suitable for manufacturing parts requiring high creep and stress rupture resistance at temperatures up to 1300°F (704°C) and high oxidation resistance at temperatures up to 1800°F (982°C).

Chemical Composition Of Inconel 718 Flanges

Grade C Mn Si S Cu Fe Ni Cr
Inconel 718 0.08 max 0.35 max 0.35 max 0.015 max 0.30 max - 50.00 - 55.00 17.00 - 21.00

Mechanical Properties Of Inconel 718 Flanges

Ultimate Tensile Strength, psi .2% Yield Strength psi Elongation % Hardness Rockwell B
135,000 70,000 45 100

Dimensions of Inconel 718 Flanges

Inconel 718-flanges-Dimensions

Size in Inch Size in mm Outer Diameter Flange Thickness Hub OD Weld Neck OD Welding Neck Length Bore RF Diameter RF Height PCD Weld Face
    A B C D E F G H I J
1/2 15 90 9.6 30 21.3 46 Refer Note 34.9 2 60.3 1.6
3/4 20 100 11.2 38 26.7 51 42.9 2 69.9 1.6
1 25 110 12.7 49 33.4 54 50.8 2 79.4 1.6
1 1/4 32 115 14.3 59 42.2 56 63.5 2 88.9 1.6
1 1/2 40 125 15.9 65 48.3 60 73 2 98.4 1.6
2 50 150 17.5 78 60.3 62 92.1 2 120.7 1.6
2 1/2 65 180 20.7 90 73 68 104.8 2 139.7 1.6
3 80 190 22.3 108 88.9 68 127 2 152.4 1.6
3 1/2 90 215 22.3 122 101.6 70 139.7 2 177.8 1.6
4 100 230 22.3 135 114.3 75 157.2 2 190.5 1.6
5 125 255 22.3 164 141.3 87 185.7 2 215.9 1.6
6 150 280 23.9 192 168.3 87 215.9 2 241.3 1.6
8 200 345 27 246 219.1 100 269.9 2 298.5 1.6
10 250 405 28.6 305 273 100 323.8 2 362 1.6
12 300 485 30.2 365 323.8 113 381 2 431.8 1.6
14 350 535 33.4 400 355.6 125 412.8 2 476.3 1.6
16 400 595 35 457 406.4 125 469.9 2 539.8 1.6
18 450 635 38.1 505 457.2 138 533.4 2 577.9 1.6
20 500 700 41.3 559 508 143 584.2 2 635 1.6
24 600 815 46.1 663 610 151 692.2 2 749.3
Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 718 Alloy Flange, covering tubes: Seamless tubes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded tubes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate thickness 0.1 to 100 mm; Plate width 10-2500 mm, Strips, Alloy round bar sizes: diameter 3-800 mm;, Flat bar sizes: thickness 2-100 mm; Width: 10-500 mm, Hexagonal bar sizes: 2-100 mm;, Wire and extruded profiles. We work with steel mills to provide customers with 625 alloy, and its products meet or exceed many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.