Inconel is commonly used in extreme environments and is available in several different grades depending on the application requirements. This article will briefly compare two of the most commonly used grades-Inconel 625 and Inconel 718-to help you choose the best material.
Key Differences 625 vs. 718
Inconel 625
• Better general corrosion resistance
• Long-term high temperature stability
Inconel 718
• Precipitation hardened
• 2x's stronger than Inconel 625
Inconel 625
Inconel 625 screws possess considerable amounts of nickel, chromium, and molybdenum making it not only strong at high temperatures but also resistant to corrosion, oxidation and carburization. One of its most notable characteristics is its ability to prevent stress, pitting and crevice corrosion cracking even when exposed to chloride ions.
Benefits
• Outstanding resistance to pitting, crevice corrosion
• Almost 100% resistance to chloride induced stress corrosion cracking
• High resistance to oxidation at elevated temperatures up to 1050°C
• Good resistance to acids, such as nitric, phosphoric, sulfuric and hydrochloric, as well as to alkalis
• Easily welded by standard shop fabrication practices
• Greater longevity at high temperatures than Inconel 718
Usage Examples
Oil and gas production where hydrogen sulfide and elementary sulfur are present, marine applications including propeller blades, submarine propulsion and other naval applications
Inconel 718
Similar to its sister 625, Inconel 718 is an age hardened version of alloy 625. Aging (or precipitation hardening) produces precipitates in the molecular structure that pins the grains of the metal in place. As a result, materials usually become significantly stronger. In the case of Inconel, 718 has exceptional strength with a yield strength that is about 2x's stronger than 625!
Benefits
• Super high strength: min ultimate tensile strength of 185ksi/min yield strength of 150ksi
• Good corrosion resistance to sour gas, HCl, H2SO4
• Outstanding weldability
Usage Examples
Gas turbine and jet engines, cryogenic storage tanks, downhole oil & gas and nuclear engineering applications.
Our factory
Our nickel-based alloy products originate from a modern precision manufacturing base. The factory is equipped with fully automated vacuum induction melting (VIM), electroslag remelting (ESR), and multi-directional forging hydraulic units, ensuring that every step from melting to forming meets aerospace-grade standards. Through a digital process control system, we achieve precise control over composition purity, grain size, and mechanical properties. Each batch of products is accompanied by traceable melting reports and third-party certifications (such as DNV-GL, ABS, aerospace standards, etc.), ensuring the authenticity and reliability of performance data.

Packaging and shipping
We adopt the highest industry standards for protective packaging: all rods/plates are treated with anti-rust protection and reinforced with waterproof film and wooden crates; precision components are packaged with custom foam dividers and vacuum sealing. Through our proprietary logistics coordination system, we promise that standard specification products will be prepared and shipped within 7-15 working days after order confirmation and technical details are finalized.