Inconel 625 Pipe vs. Inconel 718 Tubing - Which is Best for Your Application?

 
Inconel 625 Pipe And Inconel 718 Tubing
 

Gnee Steel

 

Inconel 625 vs. Inconel 718 Tubing - Which is Best for Your Application?

Both Inconel 625 pipe and Inconel 718 alloy pipe are excellent choices for piping applications, but they each have different areas of strength. Inconel 625 seamless pipe is best suited for applications that require high corrosion resistance and good weldability, while Inconel 718 round pipe is ideal for high strength and high temperature environments.

Inconel 625 vs. Inconel 718 Tubing - Which is Best for Your Application?

Gnee Steel

 

What are the advantages of Inconel 718 pipe?

Inconel 718 alloy pipe is a high-strength, corrosion-resistant nickel-based high-temperature alloy. It has excellent mechanical properties, high-temperature strength, and resistance to oxidation and corrosion. Inconel 718 round pipe is widely used in various industries such as aerospace, oil and gas, automotive, and power generation.

Inconel 718 pipe

Specifications of inconel 625 Pipe vs inconel 718 Pipe

Specification Inconel 718 Pipe Inconel 625 Pipe
Tensile Strength 135 ksi (930 MPa) 135 ksi (930 MPa)
Melting Point 2300°F (1260°C) 2350°F (1290°C)
Density 8.19 g/cm³ 8.44 g/cm³
Yield Strength 95 ksi (655 MPa) 75 ksi (517 MPa)

Inconel 625 Pipe vs 718 Pipe : Chemical Composition

There are several factors to consider when choosing between Inconel 625 pipe or Inconel 718 seamless pipe for your project. Inconel 625 pipe is primarily composed of nickel and chromium, while Inconel 718 seamless pipe contains nickel, chromium, niobium, and molybdenum. Each alloy has its own strengths and is suitable for different applications.

Inconel 625 alloy pipe is suitable for sour environments, but additional protection may be required in some cases. Inconel 718 pipe, by contrast, is more protective and easier to weld. The final choice depends on your specific needs, so it is important to understand their characteristics before making a decision.

Element Inconel 625 Pipe Composition (%) Inconel 718 Pipe Composition (%)
Nickel (Ni) 58.0 min 50.0 min
Chromium (Cr) 20.0-23.0 17.0-21.0
Molybdenum (Mo) 8.0-10.0 2.8-3.3
Niobium (Nb) + Tantalum (Ta) – 4.75-5.50
Iron (Fe) 5.0 max 0.0-21.0
Titanium (Ti) 0.40 max 0.65-1.15
Aluminum (Al) 0.40 max 0.20-0.80
Cobalt (Co) 1.0 max 1.0 max
Carbon (C) 0.10 max 0.08 max
Manganese (Mn) 0.50 max 0.35 max
Silicon (Si) 0.50 max 0.35 max
Sulfur (S) 0.015 max 0.015 max
Phosphorus (P) 0.015 max 0.015 max

Inconel 718 Pipe Properties

Property Value
Density 8.19 g/cm³
Melting Point 1260-1340°C (2300-2440°F)
Tensile Strength 1034 MPa (150 ksi)
Yield Strength 724 MPa (105 ksi)
Elongation 12%
Modulus of Elasticity 200 GPa (29.0 x 10^6 psi)
Thermal Conductivity 11.0 W/m·K (at 100°C)
Specific Heat Capacity 447 J/kg·K
Coefficient of Thermal Expansion 13.3 µm/m·K (20-100°C)
Electrical Resistivity 1.22 µΩ·m (at 21°C)

Inconel 625 Pipe Properties

Property Value
Melting Point 1290-1350°C (2350-2460°F)
Tensile Strength 827 MPa (120,000 psi)
Density 8.44 g/cm³
Yield Strength (0.2% offset) 414 MPa (60,000 psi)
Elongation 30% in 2 inches
Hardness (HRC) 20-30
Thermal Conductivity 11.5 W/m·K (70°F)
Coefficient of Thermal Expansion 13.3 µm/m-°C (20-100°C)
Specific Heat Capacity 442 J/kg·K (20°C)
Electrical Resistivity 1.29 µΩ·m (20°C)
Corrosion Resistance Excellent resistance to corrosion in many environments, including seawater, acids, and oxidizing chemicals.

Inconel 625 Pipe vs Inconel 718 Pipe : Industrial Applications

Both Inconel 625 Tube and Inconel 718 Alloy Tube are highly versatile super alloys that offer unique properties for different applications across a wide range of industries.

Aspect Inconel 625 Inconel 718
Chemical Makeup Primarily nickel and chromium, with additional Contains nickel, chromium, niobium, and molybdenum,
  elements like molybdenum and niobium. among others.
Strength Offers good strength and toughness, suitable for Provides superior strength and high-temperature
  high-temperature applications. applications, such as aircraft engines.
Corrosion Excellent corrosion resistance, particularly in Good corrosion resistance and weldability, making
Resistance acidic environments. it ideal for harsh environments.
Temperature Can withstand high temperatures, making it Exhibits excellent resistance to oxidation and
Resistance suitable for heat exchangers and chemical maintains strength at elevated temperatures.
  processing equipment.  
Gnee Steel

 

About Gnee Steel

Gnee Steel is a supplier of Inconel 625 And Inconel 718 Tubing, covering tubes: Seamless Tubes: Size: 4 - 219 mm; Thickness: 0.5 - 20 mm; Welded Tubes: Size: 5.0 - 1219.2 mm; Thickness: 0.5 - 20 mm, Plates: Plate Thickness 0.1 to 100 mm; Plate Width 10-2500 mm, Strips, Alloy Round Bar Sizes: Diameter 3-800 mm;, Flat Bar Sizes: Thickness 2-100 mm; Width: 10-500 mm, Hexagonal Bar Sizes: 2-100 mm;, Wires and Extruded Profiles. We work with steel mills to provide customers with 625 alloy that meets or exceeds many leading industry standards, including ASTM, ASME, SAE, AMS, ISO, DIN, EN and BS standards.
Gnee Steel stocks and sells Inconel 625 And Inconel 718 Tubing, Tubes, Pipes, Plates, Strips, Plates, Round Bars, Flat Bars, Forged Billets, Hexagons, Wires and Extrusions. Feel free to contact us for a quote at ss@gneesteel.com

Send Inquiry

whatsapp

Phone

E-mail

Inquiry