what is Inconel 625?
Inconel 625 is a high-performance nickel-chromium-molybdenum superalloy (UNS N06625) prized for its exceptional resistance to corrosion (especially pitting and crevice), high temperatures (up to 2000°F/1093°C), and extreme environments, offering high strength without heat treatment, excellent weldability, and resistance to chloride stress cracking, making it crucial for aerospace (jet engines), marine, and chemical processing industries.
What is the composition of Inconel 625?
Inconel 625 is a nickel-based superalloy with a main composition of nickel (approximately 58%), chromium (20-23%), molybdenum (8-10%), and niobium (3.2-3.8%), and also contains small amounts of iron, cobalt, titanium, aluminum, carbon, manganese, silicon, phosphorus, and sulfur, giving it excellent properties across a wide temperature range from extremely low temperatures to 1800°F (982°C).
| Symbol | Element | Min % | Max % |
|---|---|---|---|
| C | Carbon | - | 0.10% |
| Mn | Manganese | - | 0.50% |
| Si | Silicon | - | 0.50% |
| P | Phosphorus | - | 0.015% |
| S | Sulfur | - | 0.015% |
| Cr | Chromium | 20.00% | 23.00% |
| Mo | Molybdenum | 8.00% | 10.00% |
| Cb (Nb) | Columbium (Niobium) | 3.15% | 4.15% |
nconel 625 material properties
For Alloy N06625 grade 1 with annealed heat treatment (Annealed ≥ 871℃/1600℉), tensile strength minimum 827 Mpa (120 ksi). Yield strength min 414 Mpa 60 ksi, Elongation minimum 30%.
For N06625 grade 2 with solution annealed, TS minimum 690 Mpa (100 ksi), YS minimum 276 Mpa (40ksi), Elongation minimum 30%.
Solution annealed at 2000℉ (1093℃) minimum, with or without subsequent stabilization anneal at 1800℉ (982℃) minimum to increase resistance to sensitization.
| Property | Up to 4", incl. | Over 4" to 10", incl. |
|---|---|---|
| Tensile Strength | 120 ksi | 110 ksi |
| Yield Strength 0.2% offset | 60 ksi | 50 ksi |
| Elongation in 4D | 30% | 25% |
| Hardness | 287 Bhn max | 287 Bhn max |
What is the difference between alloy 600 and 625?
Alloy 600 does not contain molybdenum, while alloy 625 contains more than 8% molybdenum, which makes alloy 625 also have a certain resistance to reduction. This is not available in Alloy 600. Therefore, in contrast, Inconel 625 obviously has better comprehensive corrosion resistance.
inconel 625 vs 718
Inconel 625 excels in corrosion resistance, especially in marine/chemical environments, up to ~980°C, strengthening via solid solution, making it great for flexible parts; Inconel 718 offers superior high strength, high tensile/yield strength, and creep resistance up to ~700°C, achieved through precipitation hardening, ideal for demanding aerospace/turbine parts, though it has lower corrosion resistance than 625.
What is the difference between Inconel 625 and Incoloy 825?
Inconel 625 offers superior high-temperature strength and oxidation resistance due to its higher nickel and molybdenum/niobium content, making it ideal for aerospace and aggressive oxidizing/chloride environments, while Incoloy 825, with more iron and copper, provides better cost-effectiveness and enhanced resistance to reducing acids (like sulfuric) and stress corrosion cracking in less extreme chemical settings, suitable for chemical processing and oil/gas.
GNEE currently has Inconel 625 products in stock, including: plates, sheets, coils, strips, tubes, bars, and wires. In addition, we offer a variety of surface finishes for you to choose from, such as: No.1, 2B, 2D, BA, No.3, No.4, HL, No.8, sandblasting, etc.