Jan 14, 2026 Leave a message

Datasheet-For-Inconel-601-1-6-(1)-(1).pdf

Inconel 601 Round Bar Size Chart

 

Inconel 601 Round Bar Size Chart

Size in mm Average Weight
KG/MTR KG/FT
10 0.62 0.18
12 0.90 0.30
14 1.20 0.40
16 1.60 0.50
18 2.00 0.60
20 2.50 0.80
22 3.00 0.90
24 3.56 1.08
25 3.90 1.20
28 4.80 1.50
30 5.55 1.69
32 6.30 1.90
34 7.14 2.18
36 8.00 2.44
40 9.90 3.00
45 12.49 3.81
50 15.40 4.70
56 19.34 5.89
60 22.20 6.80
63 24.47 7.46
63.5 24.86 7.58
65 26.05 7.94
70 30.20 9.20
73 32.86 10.00
75 34.72 10.58
78 37.51 11.43
80 39.50 12.00
83 42.47 12.95
85 44.55 13.58
90 50.00 15.20
92 52.19 15.91
93 53.39 16.27
95 55.65 16.95
100 61.66 18.79
105 67.98 20.72
110 74.60 22.74
115 81.64 24.88
125 96.34 29.36

 

Rolling Tolerances

Size Ovality Weight Length
up to 25 mm ± 0.5 mm 25 mm to 35 mm ± 0.6 mm 35 mm to 50 mm ± 0.8 mm 50 mm to 80 mm ± 1 mm 80 mm to 100 mm ± 1.3 mm 100 mm and above ± 1.6 % of diameter. ± 75 % of total tolerance specified on the size. 10 mm to 16 mm ± 5 %
16 mm and above ± 3 %
For fixed length : ± 100 mm

 

Steel Rod Sizes and Dimension

Diameter (inches) Diameter (mm) Weight per Foot (lbs) Weight per Meter (kg)
1/4 6.35 0.167 0.249
3/8 9.52 0.376 0.561
1/2 12.7 0.668 0.994
5/8 15.88 1.043 1.552
3/4 19.05 1.502 2.237
1 25.4 2.670 3.974
1 1/4 31.75 4.170 6.202
1 1/2 38.1 6.000 8.930
2 50.8 10.680 15.900

 

Frequently Asked Questions (FAQ):

Q: What is the standard size of a round bar?

A: Round bars are available in standard sizes, including imperial units from 1/4 inch to 2 inches and metric units from 6 mm to 50 mm. Please refer to the round bar size chart provided above for details. The size you choose will depend on your project requirements. If you need more detailed information for specific applications or materials, please feel free to inquire!

Q: What is the thickness of round bar?

A: The thickness of a round bar usually refers to its diameter, which can vary significantly depending on the application and material. Round bar diameters can range from as small as 1/8 inch (3 mm) to over 12 inches (300 mm) for specialized applications. The most common sizes are typically between 1/4 inch (6 mm) and 2 inches (50 mm).

Q: How is round bar weight calculated?

A: INCOLOY 800 is a nickel-iron-chromium alloy with good strength and excellent resistance to oxidation and carburization in high-temperature environments. It is primarily used where resistance to corrosion and oxidation is required. The alloy is particularly useful for high-temperature equipment in the petrochemical industry because of its high strength and resistance to chloride-ion-induced stress corrosion cracking.

Q: What is the equivalent of INCOLOY 800H?

A: To calculate the weight of a cylindrical rod, follow these steps:

 

Measure the diameter (D): This is the thickness of the rod.
Measure the length (L): This is the length of the rod.
Determine the density (ρ): This depends on the material of the rod (e.g., steel, aluminum, etc.).
Calculate the volume (V): Use the formula for the volume of a cylinder:
V = π × (D/2)² × L
Calculate the weight: Multiply the volume by the density:
Weight = V × ρ

 

Example:
If you have a steel rod with a diameter of 50 mm, a length of 1 meter, and a density of 7850 kg/m³, the weight calculation is as follows:
Convert the diameter to meters: 50 mm = 0.05 meters.
Calculate the volume:
V = π × (0.05/2)² × 1 = π × (0.025)² × 1 ≈ 0.0019635 cubic meters
Calculate the weight:
Weight = 0.0019635 cubic meters × 7850 kg/cubic meter ≈ 15.4 kg