Product Form Thickness Width Typical Use
Plate ≥ 3/16 in. (4.8 mm) > 10 in. (250 mm) Pressure vessels, heat exchanger tube sheets, structural fabrication.
Sheet < 3/16 in. (4.8 mm) ≥ 24 in. (610 mm) Liners, baffles, fabricated enclosures, gaskets.
Strip < 3/16 in. (4.8 mm) < 24 in. (610 mm) Springs, shims, stampings, slit-to-width components.

 

Typical Industry Stock Thicknesses

 

Stock availability varies by mill program; the ranges below are typical industry stock ranges and should be confirmed against current inventory and ASTM B168 tolerance tables at quotation time.

 

Form Typical Stock Thickness
Sheet (in.) 0.025, 0.032, 0.040, 0.050, 0.063, 0.080, 0.094, 0.100, 0.125, 0.156
Sheet (mm) 0.6, 0.8, 1.0, 1.2, 1.5, 2.0, 2.5, 3.0, 4.0
Plate (in.) 3/16, 1/4, 5/16, 3/8, 1/2, 5/8, 3/4, 1, 1-1/4, 1-1/2, 2
Plate (mm) 4.8, 6.35, 8.0, 9.53, 12.7, 15.9, 19.05, 25.4, 31.8, 38.1, 50.8
Heavier plate Up to 4 in. (100 mm) available on mill order; subject to minimum quantity.

 

Corrected Weight Table (Density 8.47 g/cm³)

 

Weight per unit area: kg/m² = 8.47 × thickness (mm); lb/ft² = 44.06 × thickness (in.). The values below are calculated from the density and are directly usable for quotation and freight estimation.

 

Thickness (mm) Thickness (in.) Weight (kg/m²) Weight (lb/ft²)
0.5 0.020 4.2 0.87
1.0 0.039 8.5 1.74
2.0 0.079 16.9 3.47
3.0 0.118 25.4 5.21
4.76 (3/16) 0.1875 40.3 8.26
6.35 (1/4) 0.250 53.8 11.02
9.53 (3/8) 0.375 80.7 16.52
12.7 (1/2) 0.500 107.6 22.03
19.05 (3/4) 0.750 161.4 33.05
25.4 (1) 1.000 215.1 44.06
38.1 (1-1/2) 1.500 322.7 66.10
50.8 (2) 2.000 430.3 88.13

Example: 10 tons of 12.7 mm plate = 10,000 / 107.6 ≈ 92.9 m² of surface area - use this figure for area-based quotations (cutting, surface treatment, packaging).

 

Coil / Strip Thickness Tolerances

 

Thickness tolerance for coil and strip depends on thickness, width and tolerance class. The table below shows a typical mill tolerance pattern for nickel-alloy strip (values in mm); confirm the exact class with your supplier against ASTM B168 or the applicable EN specification before ordering.

Thickness T (mm) Width 630–1000 mm Width 1000–1250 mm Width 1250–1550 mm
0.25 ≤ T < 0.40 ±0.035 ±0.030 –
0.40 ≤ T < 0.60 ±0.035 ±0.035 –
0.60 ≤ T < 0.80 ±0.040 ±0.040 –
0.80 ≤ T < 1.00 ±0.050 ±0.040 ±0.050
1.00 ≤ T < 1.25 ±0.055 ±0.050 ±0.060
1.25 ≤ T < 1.60 ±0.060 ±0.055 ±0.060
1.60 ≤ T < 2.00 ±0.070 ±0.065 ±0.080

 

Super Alloy AL 600™ (UNS N06600)
Inconel 600 Plate
Nickel Alloy 600 Datasheet
Inconel 600 Coil
Nickel Alloy 600/ Inconel 600 (UNS N06600)
Inconel 600 Strip

 

modular-1

ss@gneesteel.com

View Inconel 600 steel plate dimensions (mm), standard plate sizes and coil sizes, coil size table, and Gnee Steel stainless steel plate dimensions.

FAQ:

Q1: What thickness range is available for Alloy 600 plate?
Per ASTM B168, plate is 3/16 in. (4.8 mm) and thicker. Typical industry stock covers 3/16 to 2 in; heavier gauges up to 4 in. are on mill order.
Confirm current stock with the supplier.

Q2: How do I convert Alloy 600 plate weight?
Weight = 8.47 x thickness (mm) kg/m2, or 44.06 x thickness (in.) lb/ft. A 1-inch plate ≈ 44.06 lb/ft2 (215.1 kg/m2).


Q3: Is the steel/aluminum gauge chart valid for Alloy 600?
No. Gauge conversion charts describe carbon steel and aluminum sheet practice. Alloy 600 sizes follow ASTM B168 decimal-inch or milmeter
thicknesses.


Q4: What is the difference between plate, sheet and strip?
Plate is 3/16 in. and over 10 in. wide; sheet is under 3/16 in. and 24 in. wide; strip is under 3/16 in and under 24 in. wide.


Q5: Which standards cover Alloy 600 coil and strip?
ASTM B168/ASME SB168 (flat products). ASTM B167 (eamless tube), ASTM B166 (rod/bar. ASTM B564 (forgings). UNS N06600, EN W.Nr2.4816. 