Inconel 600 plate offers excellent heat and corrosion resistance, high-temperature corrosion and oxidation resistance, good hot and cold processing properties, good low-temperature strength, and good hot and cold fatigue properties. It maintains high strength at 650°C and is suitable for manufacturing chemical plant components.

Inconel 600 Plate Properties

Gnee Steel

 

How high a temperature can Inconel alloy 600 withstand?

The hot working temperature range for Inconel alloy 600 is 1600–2250°F (870–1230°C). High-intensity working requires temperatures between 1900–2250°F (1040–1230°C), while light working can be performed at temperatures as low as 1600°F (870°C).

Inconel alloy 600

Inconel 600 Plate & Sheet Specification:

Size: 1000 mm x 2000 mm, 1220 mm x 2440 mm, 1500 mm x 3000 mm, 2000 mm x 2000 mm, 2000 mm x 4000 mm
Thickness: 0.1mm to 12 mm Thk
Standards: ASTM / ASME SB 168
Form: Coils, Foils, Rolls, Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)
Finish: Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)
Hardness: Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Inconel Alloy 600 Sheet & Plate Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Inconel 600 0.15 max 1.00 max 0.50 max 0.015max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

Inconel 600 Sheet & Plates Mechanical Properties

Element Density Melting Point Tensile Strength Yield Strength (0.2%Offset) Elongation
Inconel 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

Inconel 600 Plate Applications:
Inconel 600 plate is widely used in various industries, including:

Aerospace:
Due to its excellent high-temperature resistance, Inconel 600 plate is used in gas turbine engines, structural components, and exhaust systems.

Chemical Processing:
Due to its corrosion resistance and thermal stability, Inconel 600 plate is used in equipment such as heat exchangers, chemical reactors, and piping systems.

Nuclear Power:
Due to its excellent mechanical strength and corrosion resistance, Inconel 600 plate is used in nuclear reactors, steam generators, and cooling systems.

Offshore Engineering:
Due to its resistance to seawater corrosion and high temperatures, Inconel 600 plate is used in seawater piping systems, offshore drilling, and ship exhaust systems.

Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.

Send Inquiry

whatsapp

Phone

E-mail

Inquiry