Inconel 600 alloy plate
Inconel 600 Alloy Plate Properties Information
01.

Inconel 600 alloy plate properties information

Inconel 600 alloy plates combine high strength, excellent corrosion resistance, and high-temperature stability for use in a variety of demanding applications. These plates are primarily composed of nickel, chromium, and iron, with smaller amounts of other elements such as carbon, manganese, silicon, sulfur, and copper.

02.

What temperatures can Inconel alloy 600 withstand?

The hot working temperature range for Inconel alloy 600 is 1600–2250°F (870–1230°C). High-intensity working requires temperatures between 1900–2250°F (1040–1230°C), while light working can be performed at temperatures as low as 1600°F (870°C).

Inconel Alloy 600

Inconel 600 Sheets and Plates Specification

Specifications : ASTM B168 / ASME SB168

Width : 1000mm, 1219mm, 1500mm, 1800mm, 2000mm, 2500mm, 3000mm, 3500mm, etc

Length : 2000mm, 2440mm, 3000mm, 5800mm, 6000mm, etc

Thickness : 0.3 mm to 120 mm

Hardness : Soft, Hard, Half Hard, Quarter Hard, Spring Hard etc.

Finish : Hot rolled plate (HR), Cold rolled sheet (CR), 2B, 2D, BA NO(8), SATIN (Met with Plastic Coated)

Form : Plain Sheet, Shim Sheet, Strip, Flats, Blank (Circle), Ring (Flange)

Inconel Alloy 600 Sheets & Plates Chemical Composition

Grade C Mn Si S Cu Fe Ni Cr
Alloy 600 0.15 max 1.00 max 0.50 max 0.015 max 0.50 max 6.00 – 10.00 72.00 min 14.00 – 17.00

Inconel 600 Sheets & Plates Mechanical Properties

Element Density Melting Point Tensile Strengt Yield Strength (0.2%Offset) Elongation
Alloy 600 8.47 g/cm3 1413 °C (2580 °F) Psi – 95,000 , MPa – 655 Psi – 45,000 , MPa – 310 40 %

Thickness Tolerance Chart Of Nickel Alloy 600 Plate

  Tolerance over and under nominal thickness t (mm)
Width w (mm) 2.5<t <4.5 4.5<t <6.0 6.0<t <8.0 8.0<t <10.0 10.0<t <12.5 12.5<t <16.0 16.0<t <20.0 20.0<t <25.0 25.0<t <30.0 30<t <40.0
w < 1200 0.20 0.23 0.30 0.32 0.35 0.80 0.80 0.80 1.0 1.4
1200< w <1500 0.20 0.25 0.30 0.35 0.38 0.80 0.80 0.90 1.0 1.4
1500< w <1800 0.20 0.28 0.32 0.38 0.40 0.80 0.80 0.90 1.1 1.5
1800< w <2100 0.20 0.30 0.36 0.40 0.45 0.80 0.80 0.90 1.1 1.5
2100< w <2400   0.80 0.80 0.80 0.80 0.80 0.90 1.0 1.1 1.5
2400< w <2700   0.80 0.80 0.80 0.80 0.90 1.0 1.1 1.3 1.7
2700< w <3000   0.80 0.90 1.0 1.0 1.0 1.1 1.3 1.4 1.8
Gnee Steel

 

About Gnee Steel

Gnee Steel specializes in the production and sale of various nickel-based alloys, including Nickel 201, Nickel 202, Hastelloy C-276, Hastelloy C-22, Hastelloy B, Hastelloy C-4, Inconel Alloy 600, Inconel 625, Inconel 718, Inconel X-750, Incoloy Alloy 800, Incoloy 800H/HT, Incoloy 825, Monel Alloy 400, Monel K500, and high-temperature alloys. Gnee Steel's products are widely used in aerospace, chemical, electric power, automotive, and nuclear energy applications. We also offer customized alloy solutions tailored to customer needs. For alloy pricing inquiries or customized alloy solutions, please contact us for a quote at ss@gneesteel.com.