Inconel 600 Alloy Fastener Weight Table

 

Inconel 600 Alloy Fastener Weight Table

Gnee Steel also provides a fastener weight table, which is essential for determining the total weight of all fastener types (including hex bolts, hex nuts, and washers), as well as the size and type of material used. This table also provides more detailed weight data, which is crucial for engineers, builders, and manufacturers when designing and constructing structures. For example, hex bolts weigh between 32 pounds and 11,000 pounds and are available in lengths between ½ inch and 2 inches. An M10 bolt weighs 20 grams, while an M24 bolt weighs at least 428 grams. An M24 bolt weighs at least 100 grams. Hex nuts are lighter, ranging in weight from 11.50 grams for an M10 to 144.00 grams for an M24, while washers weigh between 5.00 grams.

 

Stainless Steel Fastener Nut and Bolt Sizes and Nut Weight Chart, Heavy Hex Bolt Weight Chart, Stud Bolt Weight Chart, Hex Bolt and Nut Weight Chart, Screw Fastener Weight Chart, Fastener Weight Chart PDF, Bolt Weight Chart, Nut Weight Chart (Kilograms), Nut Weight Chart, Bolt Weight Chart (Kilograms), Fastener Weight Calculator, Metric Fastener Weight Calculator, Nut Weight Chart PDF, Nut Weight Chart (mm, kg)

 

These fasteners are common in the construction, automotive, and equipment manufacturing industries for their gripping properties and tensile strength. Using non-hardened washers on these bolts and nuts prevents load concentration by reducing surface wear. Fasteners are crucial structural components because they help efficiently connect components to form assemblies and structures. Their applications range from building construction to machinery and automotive assembly.

 

Fasteners Weight Chart

Length Diameter
1⁄2" 5⁄8" 3⁄4" 7⁄8" 1" 11⁄8" 11⁄4" 13⁄8 11⁄2
1 16.5 29.4 47.0 - - - - - -
11⁄4 17.8 31.3 49.6 74.4 104 - - - -
11⁄2 19.2 33.1 52.2 78 109 148 197 - -
13⁄4 20.5 35.3 55.3 81.9 114 154 205 261 333
2 21.9 37.4 58.4 86.1 119 160 212 270 344
21⁄4 23.3 39.8 61.6 90.3 124 167 220 279 355
21⁄2 24.7 41.7 64.7 94.6 130 174 229 290 366
23⁄4 26.1 43.9 67.8 98.8 135 181 237 300 379
3 27.4 46.1 70.9 103 141 188 246 310 391
31⁄4 28.8 48.2 74 107 146 195 255 321 403
31⁄2 30.2 50.4 77.1 111 151 202 263 332 416
33⁄4 31.6 52.5 80.2 116 157 209 272 342 428
4 33 54.7 83.3 120 162 216 280 353 441
41⁄4 34.3 56.9 86.4 124 168 223 289 363 453
41⁄2 35.7 59 89.5 128 173 230 298 374 465
43⁄4 37.1 61.2 92.7 133 179 237 306 384 478
5 38.5 63.3 95.8 137 184 244 315 395 490
51⁄4 39.9 65.5 98.9 141 190 251 324 405 503
51⁄2 41.2 67.7 102 146 196 258 332 416 515
53⁄4 42.6 69.8 105 150 201 265 341 426 527
6 44 71.9 108 154 207 272 349 437 540
61⁄4 - 74.1 111 158 212 279 358 447 552
61⁄2 - 76.3 114 163 218 286 367 458 565
63⁄4 - 78.5 118 167 223 293 375 468 577
7 - 80.6 121 171 229 300 384 479 589
71⁄4 - 82.8 124 175 234 307 392 489 602
71⁄2 - 84.9 127 179 240 314 401 500 614
73⁄4 - 87.1 130 183 246 321 410 510 626
8 - 89.2 133 187 251 328 418 521 639
81⁄4 - - - 192 257 335 427 531 651
81⁄2 - - - 196 262 342 435 542 664
83⁄4 - - - - - - 444 552 676
9 - - - - - - 453 563 689
Per inch
Adder
5.5 8.6 12.4 16.9 22.1 28 34.4 42.5 49.7
F436 Round Washers 2.1 3.6 4.8 7 9.4 11.3 13.8 16.8 20