Incoloy 825 alloy introduction, performance and implementation standards
Incoloy 825 introduction:
Titanium-stabilized Incoloy 825 nickel-based alloy is a fully austenitic nickel-iron alloy with added copper and the rare metal molybdenum. Incoloy 825 nickel-based alloy is corrosion-resistant to strong acids and alkalis in oxidizing and reducing environments.
Compared with ordinary austenite, the nickel in the nickel-based alloy can make it resistant to chloride stress corrosion, and the molybdenum and copper can make it highly resistant to corrosion in reducing environments.
Chromium and molybdenum components resist chloride pitting and corrosion in various oxidizing environments. Nickel can be added to make the material more stable during welding and less susceptible to sensitization. This non-sensitizing property makes the material resistant to intergranular corrosion even when exposed to sensitizing temperature ranges. Incoloy 825 nickel-based alloy has good corrosion resistance to a variety of processing environments, including sulfuric acid, sulfurous acid, phosphoric acid, nitric acid, Hydrofluoric acid, organic acids and bases such as sodium, potassium hydroxide, acid chloride, etc.


Incoloy 825 is a titanium-stabilized, fully austenitic nickel-iron-chromium alloy with added copper and molybdenum.
The features of Incoloy 825 are:
High resistance to chloride-induced stress corrosion
Good resistance to pitting and crevice corrosion caused by chlorides
Good antioxidant and non-oxidative resistance to hot acidity
Good toughness, even in continuous operation at room temperature and high temperature, up to approximately 550°C
Incolocy 825 nickel-based alloy is resistant to acid and alkali metal corrosion under both oxidizing and reducing conditions, as the high nickel content gives the alloy good resistance to stress corrosion. Under various conditions such as sulfuric acid, hydrochloric acid, nitric acid and other strong acids, strong alkali solutions such as sodium hydroxide and potassium hydroxide, and mixed solutions such as nitric acid, hydrochloric acid and copper sulfate all show good comprehensive performance. Like Alloy 650, Incolocy 825 nickel-based alloy is effective as a heat- and corrosion-resistant material. Excellent high-temperature strength and resistance to strong acid corrosion, oxidation and carburization make this alloy widely used in various industrial and chemical equipment, which usually work in high-temperature environments that are extremely susceptible to damage.
Incoloy 825 nickel-based alloy is both a high-temperature and corrosion-resistant alloy. The main alloying elements are chromium, nickel, molybdenum, copper, aluminum, titanium, iron, etc. Among them, chromium mainly plays an antioxidant role, and other elements have the effect of strengthening grains and grain boundaries. It has high mechanical stress and good stability at high temperatures of 600 to 1000°C, so it is often used in military aviation, rocket thrusters and high-temperature components for energy conversion. Nickel-based heat-resistant alloys were developed in the late 1930s and then gradually progressed to directional crystallization and single-crystal heat-resistant alloys and powder metallurgy superalloys. In order to meet the urgent needs of the shipbuilding industry and large-scale factory gas engines, a series of corrosion-resistant, heat-resistant, and structurally stable nickel-chromium alloys were developed after the 1960s. With the update of technology, the temperature resistance of nickel-based alloys has gradually increased from 700°C to 1200°C, and is increasing at a rate of about 15°C every year. The main reasons why nickel-based alloys are widely used are: first, there are relatively many alloying elements dissolved in nickel-based alloys, and various structures are relatively stable; secondly, they can form between metal compounds called A3B type γ[Ni3(Al,Ti) ]Mutually. The coherent and regular arrangement of this compound enhances the strength of the alloy to a certain extent, making it much higher than other types of high-temperature alloys at high temperatures; it is the nickel element in nickel-based alloys that has relatively better oxidation resistance than iron and corrosion resistance.