Jan 20, 2026 Leave a message

Hastelloy C276 Forged Pipe Fittings Weight Table

 

Type

Weight (kg)

Class

1/4"

3/8"

1/2"

3/4"

1"

1 ¼"

1 ½"

2"

2 ½"

3"

4"

90° Elbows

2000

3000

6000

0.080

0.140

0.310

0.105

0.265

0.500

0.225

0.365

0.685

0.280

0.600

1.25

0.460

1.08

1.65

0.800

1.22

2.75

1.00

2.45

3.22

1.60

2.50

6.25

2.30

5.25

10.00

4.35

7.40

17.00

10.25

13.00

14.50

Street Elbows

3000

0.131

0.225

0.325

0.530

0.940

1.30

1.47

2.30

 

 

 

45° Elbows

2000

3000

6000

0.100

0.130

0.250

0.110

0.250

0.350

0.210

0.360

0.600

0.240

0.530

0.950

0.390

0.780

1.22

0.700

1.02

1.35

0.850

1.70

2.55

1.23

2.35

5.60

3.00

5.40

8.00

3.50

6.00

15.50

9.00

10.50

13.00

Tees

2000

3000

6000

0.115

0.205

0.410

0.180

0.305

0.600

0.290

0.490

0.935

0.385

0.800

1.59

0.550

1.31

2.14

0.930

1.61

3.39

1.30

3.20

4.50

1.80

3.55

10.00

3.00

6.50

13.00

5.50

9.25

19.50

14.00

17.00

18.00

Crosses

2000

3000

6000

0.140

0.220

0.450

0.190

0.400

0.700

0.335

0.630

1.16

0.420

0.990

1.80

0.750

1.63

2.50

1.15

1.97

4.10

1.45

3.70

5.20

2.25

4.90

12.30

4.50

10.50

14.00

7.15

11.50

25.00

15.00

21.70

23.00

Couplings

3000

6000

0.056

0.105

0.066

0.115

0.140

0.370

0.200

0.450

0.390

1.00

0.730

1.65

1.03

1.85

1.35

2.80

2.30

4.00

3.15

5.50

5.80

10.00

Half Couplings

3000

6000

0.028

0.053

0.033

0.058

0.070

0.185

0.110

0.225

0.195

0.500

0.365

0.830

0.510

0.920

0.660

1.40

1.15

2.00

1.57

2.75

2.90

5.00

Caps

3000

6000

0.047

0.160

0.058

0.200

0.125

0.290

0.210

0.395

0.370

0.700

0.600

1.10

0.730

1.35

1.10

2.10

2.31

3.50

3.00

4.80

4.50

7.50

Male Plugs

TQ. 3000TE. 6000
TT.

0.016

0.026

0.048

0.028

0.047

0.070

0.048

0.071

0.130

0.090

0.130

0.220

0.170

0.218

0.320

0.273

0.410

0.500

0.400

0.490

0.720

0.600

0.770

1.35

0.890

1.61

2.20

1.25

1.94

3.30

3.10

4.50

6.00

Hexagonal Bushing

6000

0.016

 

 

 

 

0.021

0.032

 

 

 

0.032

0.047

0.057

 

 

0.063

0.083

0.098

0.170

 

0.120

0.150

0.173

0.195

0.214

0.209

0.280

0.330

0.400

0.480

0.212

0.314

0.418

0.490

0.540

0.450

0.513

0.620

0.690

0.704

0.760

1.14

1.27

1.41

1.53

1.00

1.35

1.65

1.80

2.00

2.50

2.90

3.10

3.52

3.65

Hexagonal Nipples

2000 STD-XS

3000 SCH 160

6000 XXS

0.028

0.030

 

0.047

0.055

 

0.70

0.080

0.120

0.110

0.145

0.170

0.182

0.236

0.303

0.300

0.372

0.516

0.360

0.452

0.626

0.500

0.760

0.930

0.960

1.30

1.80

1.40

1.95

2.50

2.40

3.30

4.00

Unions

3000

6000

0.167

0.300

0.211

0.500

0.305

1.12

0.490

1.60

0.830

2.15

1.22

2.42

1.53

4.73

2.30

6.50

5.00

9.50

6.25

19.20

14.50

23.00

Pipe Nipples 100 mm Length

STD

XS

SCH 160

XXS

0.060

0.075

 

 

0.080

0.105

 

 

0.125

0.155

0.190

0.250

0.165

0.215

0.280

0.355

0.240

0.305

0.415

0.540

0.330

0.435

0.550

0.770

0.400

0.530

0.720

0.950

0.530

0.740

1.06

1.31

0.850

1.12

1.46

2.00

1.10

1.46

2.05

2.65

1.30

2.15

3.20

4.00

 

Weight (kg) of Hastelloy C276 forged pipe fittings

Size |
Product (Lbs)
1/8" 1/4" 3/8" 1/2" 3/4" 1" 1-1/4" 1-1/2" 2" 2-1/2" 3" 4"
90 Elbow 3000 0.09 0.08 0.12 0.22 0.33 0.53 0.84 1.08 1.68 3.2 5.38 10.95
6000 0.1 0.15 0.29 0.4 0.73 1.17 1.48 2.79 3.28      
45 Elbow 3000 0.08 0.07 0.11 0.2 0.28 0.42 0.69 0.8 1.35 2.53 5.1 9.41
6000 0.09 0.14 0.26 0.36 0.57 0.92 1.11 2.01 2.09      
Tee 3000 0.13 0.09 0.15 0.29 0.42 0.65 1.04 1.35 2.04 3.98 5.9 13.92
6000 0.14 0.2 0.43 0.56 0.94 1.49 1.93 3.37 3.95      
Cross 3000 0.16 0.13 0.2 0.35 0.47 0.73 1.12 1.58 2.25 4.37 6.69 14.58
6000 0.17 0.26 0.45 0.67 1.07 1.75 2.26 3.96 4.42      
Full Coupling 3000 0.04 0.05 0.07 0.13 0.17 0.29 0.45 0.59 0.86 1.4 1.78 2.85
6000 0.05 0.07 0.114 0.204 0.27 0.44 0.6 1.11 1.62      
Half Coupling 3000 0.04 0.05 0.07 0.13 0.21 0.3 0.34 0.66 1.09 1.63 2.1 3.71
6000 0.06 0.09 0.12 0.21 0.31 0.51 0.75 1.25 1.92      
Red Coupling 3000 .04 0.05 0.07 0.13 0.19 0.27 0.49 0.59 0.97 1.42 1.88 3.31
6000       0.24 0.33 0.65 0.75 1.2 2.12      
Cap 3000 0.03 0.04 0.07 0.1 0.16 0.25 0.45 0.59 0.96 .43 2.74 4.24
6000 0.05 0.08 0.1 0.16 0.23 0.36 0.64 0.94 1.41      
Union 3000 0.28 0.28 0.25 0.35 0.49 0.81 1.1 1.61 2.16 3.5 5.15 11.59

 

C276 alloy forged socket weld pipe fittings weight

Compliant with ANSI B16.11 and BS 3799 standards, rating 3000-6000-9000 lbs

Product Rating 1/8" 1/4" 3/8" 1/2" 3/4" 1" 1 1/4" 1 1/2" 2" 2 1/2" 3" 4"
90° Elbows 3000 lbs 0.08 0.08 0.12 0.24 0.29 0.48 0.75 0.95 1.65 2.50 4.30 9.70
6000 lbs 0.15 0.17 0.30 0.43 0.66 1.14 1.60 2.70 2.95 - - -
45° Elbows 3000 lbs 0.08 0.08 0.10 0.19 0.25 0.38 0.58 0.83 1.15 2.05 3.40 9.00
6000 lbs 0.12 0.12 0.24 0.30 0.53 0.86 1.07 1.90 2.35 - - -
Tees 3000 lbs 0.12 0.12 0.19 0.31 0.40 0.58 0.91 1.25 2.10 3.15 5.25 13.50
6000 lbs 0.21 0.21 0.40 0.56 0.91 1.41 1.75 3.56 4.10 - - -
Crosses 3000 lbs 0.14 0.14 0.21 0.34 0.47 0.80 1.25 1.50 2.23 3.95 6.50 16.00
6000 lbs 0.26 0.26 0.50 0.67 1.06 1.79 2.15 4.45 5.40 - - -
Unions 3000 lbs 0.14 0.18 0.23 0.39 0.52 0.73 1.20 1.56 2.30 5.00 7.15
Couplings 3000 lbs 0.05 0.05 0.07 0.11 0.15 0.26 0.37 0.42 0.77 1.10 1.40 2.35
6000 lbs 0.07 0.07 0.10 0.15 0.34 0.37 0.49 0.68 1.24 - - -
Caps 3000 lbs 0.03 0.04 0.06 0.14 0.18 0.30 0.51 0.65 0.92 1.40 2.50 3.50
6000lbs 0.08 0.14 0.18 0.21 0.46 0.70 0.89 1.20 - - -
Welding Boss - 0.20 0.23 0.29 0.38 0.53 0.83 1.31 1.86 - - - -

 

Nickel C276 Threaded Pipe Fittings Weight

B16.11 / BS 3799 Grade 2000-3000-6000 lbs

Product Rating 1/8" 1/4" 3/8" 1/2" 3/4" 1" 1 1/4" 1 1/2" 2" 2 1/2" 3" 4"
90° Elbows 2000 lbs 0.08 0.08 0.11 0.23 0.28 0.46 0.80 1.00 1.60 2.30 4.35 10.25
3000 lbs 0.14 0.14 0.27 0.37 0.60 1.08 1.22 2.45 2.50 5.25 7.40 13.00
6000 lbs 0.31 0.31 0.50 0.69 1.25 1.65 2.75 3.22 6.25 10.00 17.00 18.00
45° Elbows 2000 lbs 0.10 0.10 0.11 0.21 0.24 0.39 0.70 0.85 1.23 3.00 3.50 9.00
3000 lbs 0.13 0.13 0.25 0.36 0.53 0.78 1.02 1.70 2.35 5.40 6.00 10.50
6000 lbs 0.25 0.25 0.35 0.60 0.95 1.22 1.35 2.55 5.60 8.00 15.50 13.00
Tees 2000 lbs 0.12 0.12 0.18 0.29 0.39 0.55 0.93 1.30 1.80 3.00 5.50 14.00
3000 lbs 0.21 0.21 0.31 0.49 0.80 1.31 1.61 3.20 3.55 6.50 9.25 17.00
6000 lbs 0.41 0.41 0.60 0.94 1.59 2.14 3.39 4.50 10.00 13.00 19.50 18.00
Crosses 2000 lbs 0.14 0.14 0.19 0.34 0.42 0.75 1.15 1.45 2.25 4.50 7.15 15.00
3000 lbs 0.22 0.22 0.40 0.63 0.99 1.63 1.97 3.70 4.90 10.50 11.50 21.70
6000 lbs 0.45 0.45 0.70 1.16 1.80 2.50 4.10 5.20 12.30 14.00 25.00 23.00
Couplings 3000 lbs 0.05 0.05 0.06 0.14 0.20 0.39 0.73 1.03 1.35 2.30 3.15 5.80
6000 lbs 0.10 0.10 0.12 0.37 0.45 1.00 1.65 1.85 2.80 4.00 5.50 10.00
Half Couplings 3000 lbs 0.02 0.03 0.03 0.07 0.11 0.20 0.37 0.51 0.666 1.15 1.57 2.90
6000 lbs 0.04 0.05 0.06 0.19 0.23 0.50 0.83 0.92 1.40 2.00 2.75 5.00
Caps 3000 lbs 0.04 - 0.05 0.16 0.06 0.20 0.13 0.29 0.21 0.40 0.37 0.70
6000 lbs 0.60 1.10 0.73 1.35 1.10 2.10 2.31 3.50 3.00 4.80 4.50 7.50
Street Elbows 3000 lbs - 0.13 0.23 0.33 0.53 0.94 1.30 1.47 2.30 - - -
Welding Boss - 0.20 0.23 0.29 0.38 0.53 0.83 1.31 1.86 - - - -
Pipe Nipple - 100mm 3000 (XS) 0.07 0.08 0.11 0.16 0.22 0.31 0.44 0.53 0.74 1.12 1.46 2.15
  6000 (XXS) - - - 0.25 0.36 0.54 0.77 0.95 1.31 2.00 2.65 4.00
Plug - Square Head - 0.01 0.02 0.03 0.05 0.09 0.17 0.27 0.40 0.60 0.89 1.25 3.10
Plug - Round Head - 0.04 0.05 0.07 0.13 0.22 0.32 0.50 0.72 1.35 2.20 3.30 6.00
Plug - Hex Head - 0.02 0.03 0.05 0.07 0.13 0.22 0.41 0.49 0.77 1.16 1.94 4.50
Unions FF 3000 lbs 0.14 0.17 0.21 0.31 0.49 0.83 1.22 1.53 2.30 5.00 6.25 -
  6000 lbs 0.20 0.30 0.50 1.12 1.60 2.15 2.42 4.73 6.50 9.50 19.20 -
Unions MF 3000 lbs 0.16 0.21 0.27 0.46 0.61 0.99 1.55 1.90 2.90 - - -
Hex Head Bushing - 0.02 0.03 0.06 0.10 0.17 0.33 0.42 0.62 1.27 1.65 3.10 -
Hex Nipples - 0.02 0.03 0.06 0.08 0.15 0.24 0.37 0.45 - - - -
Swage Nipples Plain 0.04 0.05 0.09 0.14 0.17 0.32 0.49 0.60 0.93 - - -
Screwed - 0.17 0.22 0.29 0.33 0.50 0.75 0.95 1.60 2.10 - - -

 

modular-1

Check today's prices for Chinese Hastelloy C276 forged pipe fittings

We also supply Hastelloy C276 socket weld pipe fittings at the best prices. You can view our latest price list for Hastelloy C-22 forged pipe fittings in various sizes. Contact Gnee Steel now for the best quote on Hastelloy C22 forged elbows.

Phone: +8615824687445

Email: ss@gneesteel.com

Send Inquiry

whatsapp

Phone

E-mail

Inquiry